Rational Design for Optimizing Hybrid Thermo-triboelectric Generators Targeting Human Activities AITranslate

Korea University; Korea University; Korea Institute of Science and Technology; Korea University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Despite the rise in Internet of Things devices and mobile electronics, devising an energy harvester with sufficient time-averaged power remains a challenge when targeting human activities. Here, we report a hybrid thermo-triboelectric generator targeting human motion with systematic optimization strategies in frequency feature-size variable spaces. The device consists of bismuth telluride (Bi2Te3) tiles with polydimethylsiloxane (PDMS) layers filled in between, thereby harvesting both thermal energy and triboelectricity from human touch. Detailed heat transport analyses reveal that optimal operational frequency for thermoelectrics may be tuned on the basis of the insulation property of PDMS. Meanwhile, triboelectricity exhibits strong feature-size dependence when PDMS is interfaced with high-dielectric thermoelectric materials. The analyses establish the design guidelines for a hybrid energy harvester that outperforms the simple physical addition of constituent energy harvesters and demonstrates an average power of 3.27 μW/cm3, which is feasible to power potential applications operated by human touch at 2.5 Hz.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01426

Chinese Library Classification Number:

Citation Information:

Despite the rise in Internet of Things devices and mobile electronics, devising an energy harvester with sufficient time-averaged power remains a challenge when targeting human activities. Here, we report a hybrid thermo-triboelectric generator targeting human motion with systematic optimization strategies in frequency feature-size variable spaces. The device consists of bismuth telluride (Bi2Te3) tiles with polydimethylsiloxane (PDMS) layers filled in between, thereby harvesting both thermal energy and triboelectricity from human touch. Detailed heat transport analyses reveal that optimal operational frequency for thermoelectrics may be tuned on the basis of the insulation property of PDMS. Meanwhile, triboelectricity exhibits strong feature-size dependence when PDMS is interfaced with high-dielectric thermoelectric materials. The analyses establish the design guidelines for a hybrid energy harvester that outperforms the simple physical addition of constituent energy harvesters and demonstrates an average power of 3.27 μW/cm3, which is feasible to power potential applications operated by human touch at 2.5 Hz.

quote

GB/T 7714-2015 [1] Byungseok Seo, Youngsun Cha, Sangtae Kim, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01426.
MLA [1] Byungseok Seo, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01426.
APA [1] Byungseok Seo, Youngsun Cha, Sangtae Kim, & Wonjoon Choi. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01426
IEEE [1] Byungseok Seo, Youngsun Cha, Sangtae Kim, and Wonjoon Choi, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01426.