Steam-Assisted Chemical Vapor Deposition of Zeolitic Imidazolate Framework AITranslate

University of New South Wales; King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); King Abdullah University of Science and Technology (KAUST); University of New South Wales; Kyushu University; King Abdullah University of Science and Technology (KAUST); University of New South Wales; Chang-Gung University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Direct growth of metal–organic frameworks (MOFs) on substrates is a prerequisite to incorporating them into functional platforms and microdevices. Nevertheless, available reports mostly rely on the solvent-based routes, typically altered from processes for powder synthesis which are obstacles to the nanofabrication. Besides, although few vapor-phase growth approaches were presented, the proposed procedures required multiple steps, such as matrix deposition and post-conversion, to obtain desired MOF films on substrates. Here, we demonstrate a steam-assisted chemical vapor deposition (CVD) method to directly synthesize highly crystalline ZIF-67 thin films at the temperature <125°C. With a slow deposition rate, the ZIF-67 forms a highly oriented thin film on a c-plane sapphire substrate, indicating the growth is epitaxial. Furthermore, we demonstrate the integration of directly grown CVD ZIF-67 as the active material of chemiresistors onto microelectronic chips. The ZIF-67 chemiresistors exhibit responses to the gas molecules, which are capable of diffusing into the cage of ZIF-67 at room temperature. The proposed synthesis method of ZIF-67 thin films is simple, scalable, cost-effective, and promising for numerous applications.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.0c00026

Chinese Library Classification Number:

Citation Information:

Direct growth of metal–organic frameworks (MOFs) on substrates is a prerequisite to incorporating them into functional platforms and microdevices. Nevertheless, available reports mostly rely on the solvent-based routes, typically altered from processes for powder synthesis which are obstacles to the nanofabrication. Besides, although few vapor-phase growth approaches were presented, the proposed procedures required multiple steps, such as matrix deposition and post-conversion, to obtain desired MOF films on substrates. Here, we demonstrate a steam-assisted chemical vapor deposition (CVD) method to directly synthesize highly crystalline ZIF-67 thin films at the temperature <125°C. With a slow deposition rate, the ZIF-67 forms a highly oriented thin film on a c-plane sapphire substrate, indicating the growth is epitaxial. Furthermore, we demonstrate the integration of directly grown CVD ZIF-67 as the active material of chemiresistors onto microelectronic chips. The ZIF-67 chemiresistors exhibit responses to the gas molecules, which are capable of diffusing into the cage of ZIF-67 at room temperature. The proposed synthesis method of ZIF-67 thin films is simple, scalable, cost-effective, and promising for numerous applications.

quote

GB/T 7714-2015 [1] JingKai Huang, Noboru Saito, Yichen Cai, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00026.
MLA [1] JingKai Huang, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00026.
APA [1] JingKai Huang, Noboru Saito, Yichen Cai, Yi Wan, ChiaChin Cheng, Mengliu Li, Junjie Shi, Kaoru Tamada, Vincent C. Tung, Sean Li, & LainJong Li. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00026
IEEE [1] JingKai Huang, Noboru Saito, Yichen Cai, Yi Wan, ChiaChin Cheng, Mengliu Li, Junjie Shi, Kaoru Tamada, Vincent C. Tung, Sean Li, and LainJong Li, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00026.