Polymerization-Induced Self-Assembly (PISA) and “Host–Guest” Complexation-Directed Polymer/Gold Nanocomposites AITranslate
Abstract AITranslate
Polymer and inorganic hybrid nanocomposites are of increasing interest for a wide variety of applications; however, the preparation of these nanocomposites often requires cumbersome procedures, especially for nanocomposites with diverse morphologies. Here, we demonstrate a facile strategy for fast preparation of polymer/gold nanocomposites through “host–guest” complexation between β-cyclodextrin (β-CD) and adamantane (Ada). Synthesis of macro-RAFT agent contains β-CD moiety, followed by polymerization-induced self-assembly (PISA), provides three types of β-CD decorated polymer nano-objects with distinguished morphologies. Subsequently, by incubating these polymer nano-objects with gold nanoparticles (AuNPs) that are modified with polymer ligands containing Ada moiety, we have successfully fabricated a series of different polymer/gold nanocomposites, including AuNPs decorated polymer vesicles, polymer sphere nano-flowers, polymer sphere nano-patterns, and polymer nano-worms. This strategy opens a gate for fast preparation of polymer-based nanocomposites with desired decorations. Nanoparticles with different morphologies and compositions, bio-macromolecules and drugs molecules, etc. are all potential decorations, leading to further diversified applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.0c00043
Chinese Library Classification Number:
Citation Information:
Polymer and inorganic hybrid nanocomposites are of increasing interest for a wide variety of applications; however, the preparation of these nanocomposites often requires cumbersome procedures, especially for nanocomposites with diverse morphologies. Here, we demonstrate a facile strategy for fast preparation of polymer/gold nanocomposites through “host–guest” complexation between β-cyclodextrin (β-CD) and adamantane (Ada). Synthesis of macro-RAFT agent contains β-CD moiety, followed by polymerization-induced self-assembly (PISA), provides three types of β-CD decorated polymer nano-objects with distinguished morphologies. Subsequently, by incubating these polymer nano-objects with gold nanoparticles (AuNPs) that are modified with polymer ligands containing Ada moiety, we have successfully fabricated a series of different polymer/gold nanocomposites, including AuNPs decorated polymer vesicles, polymer sphere nano-flowers, polymer sphere nano-patterns, and polymer nano-worms. This strategy opens a gate for fast preparation of polymer-based nanocomposites with desired decorations. Nanoparticles with different morphologies and compositions, bio-macromolecules and drugs molecules, etc. are all potential decorations, leading to further diversified applications.
quote
| GB/T 7714-2015 | [1] Bo Fan, Yiyi Liu, Jing Wan, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00043. |
| MLA | [1] Bo Fan, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00043. |
| APA | [1] Bo Fan, Yiyi Liu, Jing Wan, Simon Crawford, & San H. Thang. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00043 |
| IEEE | [1] Bo Fan, Yiyi Liu, Jing Wan, Simon Crawford, and San H. Thang, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00043. |