daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

P3 type layered oxide frameworks: An appealing family of insertion materials for K-ion batteries AITranslate

India|Normandie University;Normandie University; Karlsruhe Institute of Technology (KIT); Karlsruhe Institute of Technology (KIT)
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

K-ion batteries (KIBs) offer an efficient technological alternative to the state-of-the-art Li-ion batteries (LIBs) as energy storage devices with similar chemistry, comparable energy densities, elemental economy and uniformly distributed abundant resources. Nonetheless, their practical implementation warrants robust cathode materials that can yield high gravimetric/volumetric energy density, stable cycle life, and high-rate capability. In this scenario, P3 type layered oxides form an appealing family of KIB cathodes, which includes single transition metal based KxMO2 (M = transition metals) and multiple transition metals based KxM11-yM2yO2 and KxM11-y-zM2yM3zO2 (M1, M2, M3 = transition metals). They possess easy and scalable synthesis, high reversible capacity, and adequate operating potential. The current review attempts to capture the most recent advancements in the P3 type KIB cathodes focusing on structural stability, structure–property correlation, and electrochemical performance with suggestions for further material optimization. Finally, the challenges and potential of these P3 type oxide cathodes have been addressed to guide their future research and development as intercalation materials. Graphical abstract Download : Download high-res image (172KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.coelec.2023.101216

Chinese Library Classification Number:

Citation Information:

K-ion batteries (KIBs) offer an efficient technological alternative to the state-of-the-art Li-ion batteries (LIBs) as energy storage devices with similar chemistry, comparable energy densities, elemental economy and uniformly distributed abundant resources. Nonetheless, their practical implementation warrants robust cathode materials that can yield high gravimetric/volumetric energy density, stable cycle life, and high-rate capability. In this scenario, P3 type layered oxides form an appealing family of KIB cathodes, which includes single transition metal based KxMO2 (M = transition metals) and multiple transition metals based KxM11-yM2yO2 and KxM11-y-zM2yM3zO2 (M1, M2, M3 = transition metals). They possess easy and scalable synthesis, high reversible capacity, and adequate operating potential. The current review attempts to capture the most recent advancements in the P3 type KIB cathodes focusing on structural stability, structure–property correlation, and electrochemical performance with suggestions for further material optimization. Finally, the challenges and potential of these P3 type oxide cathodes have been addressed to guide their future research and development as intercalation materials. Graphical abstract Download : Download high-res image (172KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Pawan Kumar Jha, Valérie Pralong, Maximilian Fichtner, et al. Current Opinion in Electrochemistry, 2023(38). DOI:10.1016/j.coelec.2023.101216.
MLA [1] Pawan Kumar Jha, et al., Current Opinion in Electrochemistry, no. 38, 2023, https://doi.org/10.1016/j.coelec.2023.101216.
APA [1] Pawan Kumar Jha, Valérie Pralong, Maximilian Fichtner, & Prabeer Barpanda. (2023). Current Opinion in Electrochemistry(38). https://doi.org/10.1016/j.coelec.2023.101216
IEEE [1] Pawan Kumar Jha, Valérie Pralong, Maximilian Fichtner, and Prabeer Barpanda, Current Opinion in Electrochemistry, no. 38, 2023, doi: 10.1016/j.coelec.2023.101216.