Recent advancement in carbon-based materials as sulfur hosts for rechargeable aluminum–sulfur (Al–S) batteries AITranslate

National Institute of Technology Meghalaya; National Institute of Technology Meghalaya
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Rechargeable metal-sulfur batteries have emerged as viable candidates in the race for developing economically friendly and high energy-density batteries. The composition of a general metal-sulfur battery includes a metal anode and a sulfur-containing host on the cathode. The emergence of aluminum-based metal-sulfur batteries or aluminum-sulfur batteries can be attributed to the natural abundance of aluminum, considerable reduction in production cost, and high theoretical energy density. There have been several recent articles that have highlighted the use of carbon-based materials as excellent sulfur hosts in aluminum-sulfur battery cathodes. This review aims to highlight the scope and wide array of carbon-based cathode materials that have been reported recently. We have also briefly discussed the synthetic technologies and important findings of these reports in a concise form. Graphical abstract Download : Download high-res image (227KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.coelec.2023.101222

Chinese Library Classification Number:

Citation Information:

Rechargeable metal-sulfur batteries have emerged as viable candidates in the race for developing economically friendly and high energy-density batteries. The composition of a general metal-sulfur battery includes a metal anode and a sulfur-containing host on the cathode. The emergence of aluminum-based metal-sulfur batteries or aluminum-sulfur batteries can be attributed to the natural abundance of aluminum, considerable reduction in production cost, and high theoretical energy density. There have been several recent articles that have highlighted the use of carbon-based materials as excellent sulfur hosts in aluminum-sulfur battery cathodes. This review aims to highlight the scope and wide array of carbon-based cathode materials that have been reported recently. We have also briefly discussed the synthetic technologies and important findings of these reports in a concise form. Graphical abstract Download : Download high-res image (227KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Namrata Deka, Gitish K. Dutta. Current Opinion in Electrochemistry, 2023(38). DOI:10.1016/j.coelec.2023.101222.
MLA [1] Namrata Deka, and Gitish K. Dutta. Current Opinion in Electrochemistry, no. 38, 2023, https://doi.org/10.1016/j.coelec.2023.101222.
APA [1] Namrata Deka, & Gitish K. Dutta. (2023). Current Opinion in Electrochemistry(38). https://doi.org/10.1016/j.coelec.2023.101222
IEEE [1] Namrata Deka and Gitish K. Dutta, Current Opinion in Electrochemistry, no. 38, 2023, doi: 10.1016/j.coelec.2023.101222.