In Operando Small-Angle X-ray Scattering Investigation of Nanostructured Polymer Electrolyte for Lithium-Ion Batteries AITranslate

University Road;Physik-Department, Lehrstuhl für Funktionelle Materialien;Physik-Department, Lehrstuhl für Funktionelle Materialien
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Electrochemical energy storage still presents one of the biggest challenges that society has to face by developing alternative lithium-ion batteries (LIBs) as they already satisfy important preconditions by providing the highest energy and power densities of all battery systems. Nowadays, the employed liquid electrolytes in LIBs do not merge the world’s increasing demand of safely working batteries. Here, we use a lithium salt-doped diblock copolymer electrolyte:poly(styrene)-block-poly(ethylene oxide)/bis(trifluoromethane) lithium salt, denoted PS-b-PEO/LiTFSI, as a solid-state electrolyte. The evolving nanoscale morphology of the electrolyte material in a capillary-based LIB cell is investigated using in operando small-angle X-ray scattering (SAXS). The electrolyte is sandwiched between two opposing electrodes inside of a glass capillary and investigated during cycling at 90 °C while the X-ray beam is oriented orthogonally to the ionic current. Lithium iron phosphate (LFP) is used as a cathode, while both lithium-metal and graphite anode materials are used for the investigation of the solid-state electrolytes. The ill-defined structured lithium-ion containing block copolymer electrolyte seems morphologically more favorable for cell performance, and this is independent of the choice of anode material due to better electrode/electrolyte compatibility.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b00763

Chinese Library Classification Number:

Citation Information:

Electrochemical energy storage still presents one of the biggest challenges that society has to face by developing alternative lithium-ion batteries (LIBs) as they already satisfy important preconditions by providing the highest energy and power densities of all battery systems. Nowadays, the employed liquid electrolytes in LIBs do not merge the world’s increasing demand of safely working batteries. Here, we use a lithium salt-doped diblock copolymer electrolyte:poly(styrene)-block-poly(ethylene oxide)/bis(trifluoromethane) lithium salt, denoted PS-b-PEO/LiTFSI, as a solid-state electrolyte. The evolving nanoscale morphology of the electrolyte material in a capillary-based LIB cell is investigated using in operando small-angle X-ray scattering (SAXS). The electrolyte is sandwiched between two opposing electrodes inside of a glass capillary and investigated during cycling at 90 °C while the X-ray beam is oriented orthogonally to the ionic current. Lithium iron phosphate (LFP) is used as a cathode, while both lithium-metal and graphite anode materials are used for the investigation of the solid-state electrolytes. The ill-defined structured lithium-ion containing block copolymer electrolyte seems morphologically more favorable for cell performance, and this is independent of the choice of anode material due to better electrode/electrolyte compatibility.

quote

GB/T 7714-2015 [1] Gilles E. Möhl, Ezzeldin Metwalli, Peter MüllerBuschbaum. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00763.
MLA [1] Gilles E. Möhl, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00763.
APA [1] Gilles E. Möhl, Ezzeldin Metwalli, & Peter MüllerBuschbaum. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00763
IEEE [1] Gilles E. Möhl, Ezzeldin Metwalli, and Peter MüllerBuschbaum, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00763.