daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Promoting Oxygen Evolution Reactions through Introduction of Oxygen Vacancies to Benchmark NiFe–OOH Catalysts AITranslate

The University of New South Wales; Monash University; The University of New South Wales; Swinburne University of Technology; The University of New South Wales
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Advanced electrocatalysts toward oxygen evolution reaction (OER) at high current density with low overpotential remain a significant challenge for electrochemical water splitting. Herein, NiFe-based catalysts with appropriate electronic conductivity and catalytic activity have been obtained through introduction of oxygen vacancies by a facile and economic NaBH4 reduction approach. The combined density functional theory calculations, physical characterization, and electrochemical studies disclose that the reductive treatment creates a high amount of oxygen vacancies, high active sites, and a low energy barrier for OER. The oxygen vacancy-rich catalyst yields a more than 2-fold increased current density (from 100 to 240 mA cm–2) at a low overpotential of 270 mV, accompanied by good stability under OER conditions. The approach is also broadly applicable for NiFe compounds synthesized via different methods or substrates.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b00696

Chinese Library Classification Number:

Citation Information:

Advanced electrocatalysts toward oxygen evolution reaction (OER) at high current density with low overpotential remain a significant challenge for electrochemical water splitting. Herein, NiFe-based catalysts with appropriate electronic conductivity and catalytic activity have been obtained through introduction of oxygen vacancies by a facile and economic NaBH4 reduction approach. The combined density functional theory calculations, physical characterization, and electrochemical studies disclose that the reductive treatment creates a high amount of oxygen vacancies, high active sites, and a low energy barrier for OER. The oxygen vacancy-rich catalyst yields a more than 2-fold increased current density (from 100 to 240 mA cm–2) at a low overpotential of 270 mV, accompanied by good stability under OER conditions. The approach is also broadly applicable for NiFe compounds synthesized via different methods or substrates.

quote

GB/T 7714-2015 [1] Majid Asnavandi, Yichun Yin, Yibing Li, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00696.
MLA [1] Majid Asnavandi, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00696.
APA [1] Majid Asnavandi, Yichun Yin, Yibing Li, Chenghua Sun, & Chuan Zhao. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00696
IEEE [1] Majid Asnavandi, Yichun Yin, Yibing Li, Chenghua Sun, and Chuan Zhao, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00696.