Abstract AITranslate
We report the preparation and electrocatalytic performance of silver-containing gas diffusion electrodes (GDEs) derived from a silver coordination polymer (Ag-CP). Layer-by-layer growth of the Ag-CP onto porous supports was applied to control Ag loading. Subsequent electro-decomposition of the Ag-CP resulted in highly selective and efficient CO2-to-CO GDEs in aqueous CO2 electroreduction. Afterward, the metal–organic framework (MOF)-mediated approach was transferred to a gas-fed flow electrolyzer for high current density tests. The in situ formed GDE, with a low silver loading of 0.2 mg cm–2, showed a peak performance of jCO ≈ 385 mA cm–2 at around −1.0 V vs RHE and stable operation with high FECO (>96%) at jTotal = 300 mA cm–2 over a 4 h run. These results demonstrate that the MOF-mediated approach offers a facile route for manufacturing uniformly dispersed Ag catalysts for CO2 electrochemical reduction by eliminating ill-defined deposition steps (drop-casting, etc.) while allowing control of the catalyst structure through self-assembly.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.9b01509
Chinese Library Classification Number:
Citation Information:
We report the preparation and electrocatalytic performance of silver-containing gas diffusion electrodes (GDEs) derived from a silver coordination polymer (Ag-CP). Layer-by-layer growth of the Ag-CP onto porous supports was applied to control Ag loading. Subsequent electro-decomposition of the Ag-CP resulted in highly selective and efficient CO2-to-CO GDEs in aqueous CO2 electroreduction. Afterward, the metal–organic framework (MOF)-mediated approach was transferred to a gas-fed flow electrolyzer for high current density tests. The in situ formed GDE, with a low silver loading of 0.2 mg cm–2, showed a peak performance of jCO ≈ 385 mA cm–2 at around −1.0 V vs RHE and stable operation with high FECO (>96%) at jTotal = 300 mA cm–2 over a 4 h run. These results demonstrate that the MOF-mediated approach offers a facile route for manufacturing uniformly dispersed Ag catalysts for CO2 electrochemical reduction by eliminating ill-defined deposition steps (drop-casting, etc.) while allowing control of the catalyst structure through self-assembly.
quote
| GB/T 7714-2015 | [1] Riming Wang, Henrik Haspel, Alexey Pustovarenko, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01509. |
| MLA | [1] Riming Wang, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01509. |
| APA | [1] Riming Wang, Henrik Haspel, Alexey Pustovarenko, Alla Dikhtiarenko, Artem Russkikh, Genrikh Shterk, Dmitrii Osadchii, Samy OuldChikh, Ming Ma, Wilson A. Smith, Kazuhiro Takanabe, Freek Kapteijn, & Jorge Gascon. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01509 |
| IEEE | [1] Riming Wang, Henrik Haspel, Alexey Pustovarenko, Alla Dikhtiarenko, Artem Russkikh, Genrikh Shterk, Dmitrii Osadchii, Samy OuldChikh, Ming Ma, Wilson A. Smith, Kazuhiro Takanabe, Freek Kapteijn, and Jorge Gascon, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01509. |