Charge Localization, Stabilization, and Hopping in Lead Halide Perovskites: Competition between Polaron Stabilization and Cation Disorder AITranslate

Computational Laboratory for Hybrid/Organic Photovoltaics (CLHYO);Computational Laboratory for Hybrid/Organic Photovoltaics (CLHYO);Computational Laboratory for Hybrid/Organic Photovoltaics (CLHYO); University of Perugia
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Metal halide perovskites, of general formula ABX3, show a complex interplay of the inorganic BX3 sublattice and the organic/inorganic A-site cations, which likely determines some of their peculiar optoelectronic properties. Comprehension of the physics underlying this interaction may reveal further means of fine-tuning their optoelectronic response. Here, we investigate in depth charge–lattice interactions associated with the formation of polarons in different models of the prototypical CH3NH3PbI3 perovskite through advanced electronic structure calculations. We demonstrate that charge localization, while induced by the disordered dipolar field of the organic cations, is stabilized by distortions in the inorganic sublattice. Polaron hopping between neighboring minima is related to the random reorientation of the organic cations and occurs via a delocalized transition state. Our simulations highlight a struggle between thermally induced disorder, driven by the motion of A-site cations, and polaron stabilization within the BX3 sublattice, which explains the simultaneous low mobility and high diffusion length of charge carriers in lead halide perovskites.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01353

Chinese Library Classification Number:

Citation Information:

Metal halide perovskites, of general formula ABX3, show a complex interplay of the inorganic BX3 sublattice and the organic/inorganic A-site cations, which likely determines some of their peculiar optoelectronic properties. Comprehension of the physics underlying this interaction may reveal further means of fine-tuning their optoelectronic response. Here, we investigate in depth charge–lattice interactions associated with the formation of polarons in different models of the prototypical CH3NH3PbI3 perovskite through advanced electronic structure calculations. We demonstrate that charge localization, while induced by the disordered dipolar field of the organic cations, is stabilized by distortions in the inorganic sublattice. Polaron hopping between neighboring minima is related to the random reorientation of the organic cations and occurs via a delocalized transition state. Our simulations highlight a struggle between thermally induced disorder, driven by the motion of A-site cations, and polaron stabilization within the BX3 sublattice, which explains the simultaneous low mobility and high diffusion length of charge carriers in lead halide perovskites.

quote

GB/T 7714-2015 [1] Francesco Ambrosio, Daniele Meggiolaro, Edoardo Mosconi, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01353.
MLA [1] Francesco Ambrosio, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01353.
APA [1] Francesco Ambrosio, Daniele Meggiolaro, Edoardo Mosconi, & Filippo De Angelis. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01353
IEEE [1] Francesco Ambrosio, Daniele Meggiolaro, Edoardo Mosconi, and Filippo De Angelis, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01353.