daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Nature-Inspired Heat and Moisture Exchanger Filters Composed of Gelatin and Chitosan for the Design of Eco-Sustainable “Artificial Noses” AITranslate

Institute of Science;Institute of Science;Pollution S.r.l.;Institute of Atmospheric Sciences and Climate (ISAC-CNR);Institute of Atmospheric Sciences and Climate (ISAC-CNR); University of Ferrara;Pollution S.r.l.;Institute of Science;Institute of Science
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

For long-term mechanical ventilation, during anesthesia or intensive care, it is crucial to preserve a minimum level of humidity to avoid damage to the respiratory epithelium. Heat and moisture exchange filters (HME), also called “artificial noses,” are passive systems that contribute to delivering inspired gases at about the same conditions of healthy respiration, i.e., 32 °C and relative humidity higher than 90%. Current HME devices suffer from limitations linked either to performance and filtration efficiency to their inadequate antibacterial efficiency, sterilization methods, and durability. Furthermore, in times of global warming and diminishing petroleum oil reserves, replacing the employing of synthetic materials with biomass biodegradable raw materials has considerable economic and environmental value. In the present study, a generation of eco-sustainable, bioinspired, and biodegradable HME devices are designed and developed through a green-chemistry process based on raw materials deriving from food waste and taking inspiration from the functioning, structure, and chemistry of our respiratory system. In particular, different blends are obtained by mixing aqueous solutions of gelatin and chitosan in various polymer ratios and concentrations and then by cross-linking them with different low amounts of genipin, a natural chemical cross-linker. Finally, the blends, post-gelation, are freeze-dried to obtain three-dimensional (3D) highly porous aerogels reproducing both the highly exposed surface area of the upper respiratory ways and the chemical composition of the mucus secretion covering the nasal mucosae. Results are comparable with accepted standards for HME devices and suitable bacteriostatic potential, thus validating these bioinspired materials as promising candidates to be used as an eco-sustainable generation of HME devices.

KeyWords AITranslate

green chemistry bioinspired material HME device circular economy bacteriostatic
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00140

Chinese Library Classification Number:

Citation Information:

For long-term mechanical ventilation, during anesthesia or intensive care, it is crucial to preserve a minimum level of humidity to avoid damage to the respiratory epithelium. Heat and moisture exchange filters (HME), also called “artificial noses,” are passive systems that contribute to delivering inspired gases at about the same conditions of healthy respiration, i.e., 32 °C and relative humidity higher than 90%. Current HME devices suffer from limitations linked either to performance and filtration efficiency to their inadequate antibacterial efficiency, sterilization methods, and durability. Furthermore, in times of global warming and diminishing petroleum oil reserves, replacing the employing of synthetic materials with biomass biodegradable raw materials has considerable economic and environmental value. In the present study, a generation of eco-sustainable, bioinspired, and biodegradable HME devices are designed and developed through a green-chemistry process based on raw materials deriving from food waste and taking inspiration from the functioning, structure, and chemistry of our respiratory system. In particular, different blends are obtained by mixing aqueous solutions of gelatin and chitosan in various polymer ratios and concentrations and then by cross-linking them with different low amounts of genipin, a natural chemical cross-linker. Finally, the blends, post-gelation, are freeze-dried to obtain three-dimensional (3D) highly porous aerogels reproducing both the highly exposed surface area of the upper respiratory ways and the chemical composition of the mucus secretion covering the nasal mucosae. Results are comparable with accepted standards for HME devices and suitable bacteriostatic potential, thus validating these bioinspired materials as promising candidates to be used as an eco-sustainable generation of HME devices.

quote

GB/T 7714-2015 [1] Elisabetta Campodoni, Chiara Artusi, Brais Vazquez Iglesias, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00140.
MLA [1] Elisabetta Campodoni, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00140.
APA [1] Elisabetta Campodoni, Chiara Artusi, Brais Vazquez Iglesias, Alessia Nicosia, Franco Belosi, Alberta Vandini, Paolo Monticelli, Anna Tampieri, & Monica Sandri. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00140
IEEE [1] Elisabetta Campodoni, Chiara Artusi, Brais Vazquez Iglesias, Alessia Nicosia, Franco Belosi, Alberta Vandini, Paolo Monticelli, Anna Tampieri, and Monica Sandri, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00140. keywords: {green chemistry;bioinspired material;HME device;circular economy;bacteriostatic}