A new approach for characterizing internal stress of fresh concrete during thermal treatment period AITranslate

Central South University; The Hong Kong Polytechnic University; Central South University; Central South University; Central South University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Addressing the scarcity of research on the residual expansion deformation of steam-cured concrete and its underlying factors, this study introduces a testing apparatus to characterize the internal stress in fresh concrete during the thermal treatment. It explores the impact of water-to-cement ratio (w/c) and paste-to-aggregate ratio (p/a) on internal stress and elucidates the developmental patterns of internal stress in concrete throughout the thermal treatment phase. The key findings are as follows: (i) During the thermal treatment, the internal stress in concrete under constraint is predominantly compressive, exhibiting a rapid increase in the heating stage, followed by a gradual decline in the constant temperature treatment stage, and a continued decrease with a decelerating trend during the cooling stage. (ii) Both w/c and p/c significantly influence internal stress in concrete, and this stress can be enhanced by reducing the initial free water content and augmenting the initial structural strength of the concrete. This paper serves as a valuable foundation and reference for further investigations into the residual expansion deformation of steam-cured concrete.

KeyWords AITranslate

Fresh concrete Thermal treatment Internal stress Characterization
No data

Basic Information:

DOI:https://doi.org/10.1016/j.cscm.2023.e02708

Chinese Library Classification Number:

Citation Information:

Addressing the scarcity of research on the residual expansion deformation of steam-cured concrete and its underlying factors, this study introduces a testing apparatus to characterize the internal stress in fresh concrete during the thermal treatment. It explores the impact of water-to-cement ratio (w/c) and paste-to-aggregate ratio (p/a) on internal stress and elucidates the developmental patterns of internal stress in concrete throughout the thermal treatment phase. The key findings are as follows: (i) During the thermal treatment, the internal stress in concrete under constraint is predominantly compressive, exhibiting a rapid increase in the heating stage, followed by a gradual decline in the constant temperature treatment stage, and a continued decrease with a decelerating trend during the cooling stage. (ii) Both w/c and p/c significantly influence internal stress in concrete, and this stress can be enhanced by reducing the initial free water content and augmenting the initial structural strength of the concrete. This paper serves as a valuable foundation and reference for further investigations into the residual expansion deformation of steam-cured concrete.

quote

GB/T 7714-2015 [1] Yu Xiang, Jionghuang He, Guangcheng Long, et al. Case Studies in Construction Materials, 2024(20). DOI:10.1016/j.cscm.2023.e02708.
MLA [1] Yu Xiang, et al., Case Studies in Construction Materials, no. 20, 2024, https://doi.org/10.1016/j.cscm.2023.e02708.
APA [1] Yu Xiang, Jionghuang He, Guangcheng Long, Youjun Xie, & Jilin Wang. (2024). Case Studies in Construction Materials(20). https://doi.org/10.1016/j.cscm.2023.e02708
IEEE [1] Yu Xiang, Jionghuang He, Guangcheng Long, Youjun Xie, and Jilin Wang, Case Studies in Construction Materials, no. 20, 2024, doi: 10.1016/j.cscm.2023.e02708. keywords: {Fresh concrete;Thermal treatment;Internal stress;Characterization}