Interfacial Hydrogen Spillover on Pd-TiO2 with Oxygen Vacancies Promotes Formate Electrooxidation AITranslate

Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology; Beijing University of Chemical Technology;Institute of High Energy Physics; University of New South Wales; Beijing University of Chemical Technology; Beijing University of Chemical Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Pd-based catalysts are crucial in direct formate fuel cells owing to their high stability and selectivity for the formate oxidation reaction (FOR) to CO2, avoiding carbonaceous poisoning species (e.g., COad, CHx) in alkaline media. However, the kinetics of Pd-based electrocatalysts are considerably impeded by the unfavorable adsorption of hydrogen species (Had), which serve as the primary intermediators and occlude the active sites. Herein, we crafted electron-rich Pd nanoparticles on a TiO2 support with oxygen vacancies (Pd/Ov-TiO2) to improve Had desorption. The as-prepared Pd/Ov-TiO2 exhibited a high mass activity of 4.16 A mgPd–1, outperforming Pd/TiO2 without oxygen vacancies and commercial Pd/C by 1.41 and 2.72 times, respectively. Experimental characterizations and density functional theory calculations revealed that the oxygen-vacant TiO2 can concurrently downshift the d-band center of Pd and facilitate hydrogen spillover, thereby accelerating Had desorption and FOR kinetics. Our findings provide a strategy to refine Pd-based catalysts for broader electrochemical uses.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c01426

Chinese Library Classification Number:

Citation Information:

Pd-based catalysts are crucial in direct formate fuel cells owing to their high stability and selectivity for the formate oxidation reaction (FOR) to CO2, avoiding carbonaceous poisoning species (e.g., COad, CHx) in alkaline media. However, the kinetics of Pd-based electrocatalysts are considerably impeded by the unfavorable adsorption of hydrogen species (Had), which serve as the primary intermediators and occlude the active sites. Herein, we crafted electron-rich Pd nanoparticles on a TiO2 support with oxygen vacancies (Pd/Ov-TiO2) to improve Had desorption. The as-prepared Pd/Ov-TiO2 exhibited a high mass activity of 4.16 A mgPd–1, outperforming Pd/TiO2 without oxygen vacancies and commercial Pd/C by 1.41 and 2.72 times, respectively. Experimental characterizations and density functional theory calculations revealed that the oxygen-vacant TiO2 can concurrently downshift the d-band center of Pd and facilitate hydrogen spillover, thereby accelerating Had desorption and FOR kinetics. Our findings provide a strategy to refine Pd-based catalysts for broader electrochemical uses.

quote

GB/T 7714-2015 [1] Zheng Tang, Yongjia Li, Kaixin Zhang, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01426.
MLA [1] Zheng Tang, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01426.
APA [1] Zheng Tang, Yongjia Li, Kaixin Zhang, Xiaoxuan Wang, Shiyu Wang, Yanfei Sun, Huiying Zhang, Shuyuan Li, Jinrui Wang, Xueying Gao, Zishan Hou, Lanlan Shi, Zhi Yuan, Kaiqi Nie, Jiangzhou Xie, Zhiyu Yang, & YiMing Yan. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01426
IEEE [1] Zheng Tang, Yongjia Li, Kaixin Zhang, Xiaoxuan Wang, Shiyu Wang, Yanfei Sun, Huiying Zhang, Shuyuan Li, Jinrui Wang, Xueying Gao, Zishan Hou, Lanlan Shi, Zhi Yuan, Kaiqi Nie, Jiangzhou Xie, Zhiyu Yang, and YiMing Yan, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01426.