daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Enhancing Intermolecular Interaction of Spiro-OMeTAD for Stable Perovskite Solar Cells with Efficiencies over 24% AITranslate

Yonsei University;University of Angers; CNRS-Yonsei University; CNRS-Yonsei University;University of Angers;Pohang Accelerator Laboratory; Yonsei University; Sungkyunkwan University; CNRS-Yonsei University; Yonsei University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The organic nature of 2,2′,7,7′-tetrakis(N,N-di-p-methoxyphenylamine)-9,9′-spirobifluorene (spiro-OMeTAD) has been noted as a stability-limiting factor in perovskite solar cells (PSCs). The requirement for a hygroscopic dopant (lithium bis(trifluoromethanesulfonyl)imide) and low doping efficiency further contribute to the role of spiro-OMeTAD in the easy degradation of PSCs. To resolve this issue, we report a simple strategy enabling the efficiency of spiro-OMeTAD-based PSCs to reach over 24% while greatly enhancing their operational stability. Three different tris(4-methoxyphenyl)amine coupled materials (TCMs) with different core units were synthesized and added in the spiro-OMeTAD hole-transporting layers (HTLs) resulting in enhanced intermolecular interactions. When each TCM was added to spiro-OMeTAD (5 mol % to spiro-OMeTAD), the highest PCE of over 24% was maintained over 90% during 1200 h of operation without encapsulation. This strategy enabled an intermolecular interaction route within the HTL that facilitates efficient hole transport and decreases the amount of dopant needed, which are key parameters for operational stability enhancement.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c01016

Chinese Library Classification Number:

Citation Information:

The organic nature of 2,2′,7,7′-tetrakis(N,N-di-p-methoxyphenylamine)-9,9′-spirobifluorene (spiro-OMeTAD) has been noted as a stability-limiting factor in perovskite solar cells (PSCs). The requirement for a hygroscopic dopant (lithium bis(trifluoromethanesulfonyl)imide) and low doping efficiency further contribute to the role of spiro-OMeTAD in the easy degradation of PSCs. To resolve this issue, we report a simple strategy enabling the efficiency of spiro-OMeTAD-based PSCs to reach over 24% while greatly enhancing their operational stability. Three different tris(4-methoxyphenyl)amine coupled materials (TCMs) with different core units were synthesized and added in the spiro-OMeTAD hole-transporting layers (HTLs) resulting in enhanced intermolecular interactions. When each TCM was added to spiro-OMeTAD (5 mol % to spiro-OMeTAD), the highest PCE of over 24% was maintained over 90% during 1200 h of operation without encapsulation. This strategy enabled an intermolecular interaction route within the HTL that facilitates efficient hole transport and decreases the amount of dopant needed, which are key parameters for operational stability enhancement.

quote

GB/T 7714-2015 [1] Jung Hwan Lee, Tatiana Ghanem, Darío Javier Puchán Sánchez, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c01016.
MLA [1] Jung Hwan Lee, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c01016.
APA [1] Jung Hwan Lee, Tatiana Ghanem, Darío Javier Puchán Sánchez, Pierre Josse, Philippe Blanchard, Hyungju Ahn, Dominik Lungerich, NamGyu Park, Clément Cabanetos, & Jong Hyeok Park. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c01016
IEEE [1] Jung Hwan Lee, Tatiana Ghanem, Darío Javier Puchán Sánchez, Pierre Josse, Philippe Blanchard, Hyungju Ahn, Dominik Lungerich, NamGyu Park, Clément Cabanetos, and Jong Hyeok Park, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c01016.