Abstract AITranslate

The prediction of the morphology of wet-spun fibers has so far been only possible by complex and experimentally intensive approaches that include the construction of ternary phase diagrams. Ultimately, however, the available models give approximate information. Here we propose an alternative predictive approach that uses design principles based on the combination of (1) relative energy difference (RED) of Hansen solubility and (2) a kinetic parameter “T” that considers mass transfer effects. Such a model is applied and experimentally validated for a priori determination of the diameter and internal morphology of wet-spun fibers. Remarkably, only three variables relevant to wet-spinning are needed, namely, the choice of polymer, solvent, and nonsolvent types. A combination of systems is tested, and the morphology of the obtained fibers is determined via electron microscopy. Aspects related to demixing, internal specific surface area (BET), and layer formation on the fibers are described qualitatively. The facile implementation of the design parameters is further confirmed through comparison with data published on the subject. Our proposed model is expected to accelerate future developments in nanomaterials, especially in the context of ongoing efforts related to fiber spinning with biopolymers.

KeyWords AITranslate

wetspinning macrovoids microcellular delayed instantaneous demixing
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00089

Chinese Library Classification Number:

Citation Information:

The prediction of the morphology of wet-spun fibers has so far been only possible by complex and experimentally intensive approaches that include the construction of ternary phase diagrams. Ultimately, however, the available models give approximate information. Here we propose an alternative predictive approach that uses design principles based on the combination of (1) relative energy difference (RED) of Hansen solubility and (2) a kinetic parameter “T” that considers mass transfer effects. Such a model is applied and experimentally validated for a priori determination of the diameter and internal morphology of wet-spun fibers. Remarkably, only three variables relevant to wet-spinning are needed, namely, the choice of polymer, solvent, and nonsolvent types. A combination of systems is tested, and the morphology of the obtained fibers is determined via electron microscopy. Aspects related to demixing, internal specific surface area (BET), and layer formation on the fibers are described qualitatively. The facile implementation of the design parameters is further confirmed through comparison with data published on the subject. Our proposed model is expected to accelerate future developments in nanomaterials, especially in the context of ongoing efforts related to fiber spinning with biopolymers.

quote

GB/T 7714-2015 [1] Anurodh Tripathi, Marius Rutkevičius, Arnab Bose, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00089.
MLA [1] Anurodh Tripathi, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00089.
APA [1] Anurodh Tripathi, Marius Rutkevičius, Arnab Bose, Orlando J. Rojas, & Saad A. Khan. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00089
IEEE [1] Anurodh Tripathi, Marius Rutkevičius, Arnab Bose, Orlando J. Rojas, and Saad A. Khan, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00089. keywords: {wetspinning;macrovoids;microcellular;delayed;instantaneous demixing}