Hydrogen-Bond Driven Self-Assembly of Two-Dimensional Supramolecular Melamine-Cyanuric Acid Crystals and Its Self-Alignment in Polymer Composites for Enhanced Thermal Conduction AITranslate

The University of Akron; The University of Akron; Northwestern Polytechnical University; Northwestern Polytechnical University; The University of Akron; The University of Akron; University of Akron; The University of Akron
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Polymer composites are of great interest in thermal conduction applications, while poor filler dispersion and enormous phonon scattering at composite interface become the critical bottleneck for efficient thermal conduction. This work presents a multiple hydrogen bonded supramolecular crystal, melamine-cyanurate (MC), with remarkable potential to develop self-assembled 2-D layered sheet structures while at the same time strengthening thermal interfaces. Such a composite is prepared by an in situ coprecipitation method resulting in homogeneous distribution of MC crystals. An extensive network of multiple hydrogen bonds present in this supramolecular assembly along with aligned layered structure facilitated efficient phonon transport. As a result, 65% enhancement of TC can be achieved by incorporating 2D MC crystals in the composites. The mechanism of MC crystal assembling and orientation in the composite are discussed as well. Overall this work offers a new strategy for the design and development of thermally conductive materials via supramolecular assembling.

KeyWords AITranslate

polymer supramolecular assembly thermal conductivity phonon hydrogen bonding
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00111

Chinese Library Classification Number:

Citation Information:

Polymer composites are of great interest in thermal conduction applications, while poor filler dispersion and enormous phonon scattering at composite interface become the critical bottleneck for efficient thermal conduction. This work presents a multiple hydrogen bonded supramolecular crystal, melamine-cyanurate (MC), with remarkable potential to develop self-assembled 2-D layered sheet structures while at the same time strengthening thermal interfaces. Such a composite is prepared by an in situ coprecipitation method resulting in homogeneous distribution of MC crystals. An extensive network of multiple hydrogen bonds present in this supramolecular assembly along with aligned layered structure facilitated efficient phonon transport. As a result, 65% enhancement of TC can be achieved by incorporating 2D MC crystals in the composites. The mechanism of MC crystal assembling and orientation in the composite are discussed as well. Overall this work offers a new strategy for the design and development of thermally conductive materials via supramolecular assembling.

quote

GB/T 7714-2015 [1] Nitin Mehra, Madelyn Jeske, Xutong Yang, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00111.
MLA [1] Nitin Mehra, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00111.
APA [1] Nitin Mehra, Madelyn Jeske, Xutong Yang, Junwei Gu, Marjan Alsadat Kashfipour, Yifan Li, Jessi Alan Baughman, & Jiahua Zhu. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00111
IEEE [1] Nitin Mehra, Madelyn Jeske, Xutong Yang, Junwei Gu, Marjan Alsadat Kashfipour, Yifan Li, Jessi Alan Baughman, and Jiahua Zhu, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00111. keywords: {polymer;supramolecular assembly;thermal conductivity;phonon;hydrogen bonding}