Standard layer-by-layer solution processing methods constrain lead–halide perovskite device architectures. The layer below the perovskite must be robust to the strong organic solvents used to form the perovskite while the layer above has a limited thermal budget and must be processed in nonpolar solvents to prevent perovskite degradation. To circumvent these limitations, we developed a procedure where two transparent conductive oxide/transport material/perovskite half stacks are independently fabricated and then laminated together at the perovskite/perovskite interface. Using ultraviolet–visible absorption spectroscopy, external quantum efficiency, X-ray diffraction, and time-resolved photoluminesence spectroscopy, we show that this procedure improves photovoltaic properties of the perovskite layer. Applying this procedure, semitransparent devices employing two high-temperature oxide transport layers were fabricated, which realized an average efficiency of 9.6% (maximum: 10.6%) despite series resistance limitations from the substrate design. Overall, the developed lamination procedure curtails processing constraints, enables new device designs, and affords new opportunities for optimization.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b00548
Chinese Library Classification Number:
Citation Information:
Standard layer-by-layer solution processing methods constrain lead–halide perovskite device architectures. The layer below the perovskite must be robust to the strong organic solvents used to form the perovskite while the layer above has a limited thermal budget and must be processed in nonpolar solvents to prevent perovskite degradation. To circumvent these limitations, we developed a procedure where two transparent conductive oxide/transport material/perovskite half stacks are independently fabricated and then laminated together at the perovskite/perovskite interface. Using ultraviolet–visible absorption spectroscopy, external quantum efficiency, X-ray diffraction, and time-resolved photoluminesence spectroscopy, we show that this procedure improves photovoltaic properties of the perovskite layer. Applying this procedure, semitransparent devices employing two high-temperature oxide transport layers were fabricated, which realized an average efficiency of 9.6% (maximum: 10.6%) despite series resistance limitations from the substrate design. Overall, the developed lamination procedure curtails processing constraints, enables new device designs, and affords new opportunities for optimization.
quote
| GB/T 7714-2015 | [1] Sean P. Dunfield, David T. Moore, Talysa R. Klein, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00548. |
| MLA | [1] Sean P. Dunfield, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00548. |
| APA | [1] Sean P. Dunfield, David T. Moore, Talysa R. Klein, David M. Fabian, Jeffrey A. Christians, Alex G. Dixon, Benjia Dou, Shane Ardo, Matthew C. Beard, Sean E. Shaheen, Joseph J. Berry, & Maikel F. A. M. van Hest. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00548 |
| IEEE | [1] Sean P. Dunfield, David T. Moore, Talysa R. Klein, David M. Fabian, Jeffrey A. Christians, Alex G. Dixon, Benjia Dou, Shane Ardo, Matthew C. Beard, Sean E. Shaheen, Joseph J. Berry, and Maikel F. A. M. van Hest, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00548. |