p-Block Antimony Single-Atom Catalysts for Nitric Oxide Electroreduction to Ammonia AITranslate
Abstract AITranslate
Electrocatalytic NO reduction to NH3 (NORR) offers a prospective approach to attain both harmful NO removal and efficient NH3 electrosynthesis. Main-group p-block metals are promising NORR candidates but still lack adequate exploration. Herein, p-block Sb single atoms confined in amorphous MoO3 (Sb1/a-MoO3) are designed as an efficient NORR catalyst, exhibiting the highest NH3 yield rate of 273.5 μmol h–1 cm–2 and a NO-to-NH3 Faradaic efficiency of 91.7% at −0.6 V vs RHE. In situ spectroscopic characterizations and theoretical computations reason that the outstanding NORR performance of Sb1/a-MoO3 arises from the isolated Sb1 sites, which can optimize the adsorption of *NO/*NHO to lower the reaction energy barriers and simultaneously exhibit a higher affinity to NO than to H2O/H species. Moreover, our strategy can be extended to prepare Bi1/a-MoO3, showing a high NORR property, demonstrating the immense potential of p-block metal single-atom catalysts toward the high-performing NORR electrocatalysis.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.2c02882
Chinese Library Classification Number:
Citation Information:
Electrocatalytic NO reduction to NH3 (NORR) offers a prospective approach to attain both harmful NO removal and efficient NH3 electrosynthesis. Main-group p-block metals are promising NORR candidates but still lack adequate exploration. Herein, p-block Sb single atoms confined in amorphous MoO3 (Sb1/a-MoO3) are designed as an efficient NORR catalyst, exhibiting the highest NH3 yield rate of 273.5 μmol h–1 cm–2 and a NO-to-NH3 Faradaic efficiency of 91.7% at −0.6 V vs RHE. In situ spectroscopic characterizations and theoretical computations reason that the outstanding NORR performance of Sb1/a-MoO3 arises from the isolated Sb1 sites, which can optimize the adsorption of *NO/*NHO to lower the reaction energy barriers and simultaneously exhibit a higher affinity to NO than to H2O/H species. Moreover, our strategy can be extended to prepare Bi1/a-MoO3, showing a high NORR property, demonstrating the immense potential of p-block metal single-atom catalysts toward the high-performing NORR electrocatalysis.
quote
| GB/T 7714-2015 | [1] Kai Chen, Ying Zhang, Jiaqi Xiang, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02882. |
| MLA | [1] Kai Chen, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02882. |
| APA | [1] Kai Chen, Ying Zhang, Jiaqi Xiang, Xiaolin Zhao, Xingang Li, & Ke Chu. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02882 |