daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Coalescing Cation Selectivity Approaches in Ionomers AITranslate

Lawrence Berkeley National Laboratory;Lawrence Berkeley National Laboratory;Lawrence Berkeley National Laboratory
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Inconsistent selectivity measures used in the literature to quantify an ionomer’s preference for one ion over another make it challenging to compare uptake of different ions across studies. Preferential ion-partitioning, which leads to partially exchanged membranes, needs to be studied to gain a fundamental understanding of the nature of ion/membrane interactions as well as to begin to unravel how varying ion fractions, whether or not intentional, may affect the membrane’s properties and thus durability and performance. In this focus review, we use Nafion as a prototypical example to explore partial exchange studies and codify the various literature experiments and theory into a comprehensive whole, enabling formation of ionomer databases. A few representative approaches to selectivity are dissected to identify the points of divergence between them as well as to re-examine the embedded assumptions therein. Lastly, modeling strategies for ion selectivity of the membrane are reviewed to arrive at and correlate fundamental ion properties to ionomer selectivity.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00163

Chinese Library Classification Number:

Citation Information:

Inconsistent selectivity measures used in the literature to quantify an ionomer’s preference for one ion over another make it challenging to compare uptake of different ions across studies. Preferential ion-partitioning, which leads to partially exchanged membranes, needs to be studied to gain a fundamental understanding of the nature of ion/membrane interactions as well as to begin to unravel how varying ion fractions, whether or not intentional, may affect the membrane’s properties and thus durability and performance. In this focus review, we use Nafion as a prototypical example to explore partial exchange studies and codify the various literature experiments and theory into a comprehensive whole, enabling formation of ionomer databases. A few representative approaches to selectivity are dissected to identify the points of divergence between them as well as to re-examine the embedded assumptions therein. Lastly, modeling strategies for ion selectivity of the membrane are reviewed to arrive at and correlate fundamental ion properties to ionomer selectivity.

quote

GB/T 7714-2015 [1] Priyamvada Goyal, Ahmet Kusoglu, Adam Z. Weber. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00163.
MLA [1] Priyamvada Goyal, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00163.
APA [1] Priyamvada Goyal, Ahmet Kusoglu, & Adam Z. Weber. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00163
IEEE [1] Priyamvada Goyal, Ahmet Kusoglu, and Adam Z. Weber, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00163.