Stabilizing α-Phase FAPbI3 Perovskite Induced by an Ordered Solvated Quasi-Crystalline PbI2 AITranslate
Abstract AITranslate
In the two-step procedure for preparing a perovskite film, the chemistry of the PbI2 solution plays an important role in determining the phase stability of perovskite films. We report here sulfoxonium salt-controlled crystallization for stabilizing α-phase formamidinium lead iodide (FAPbI3) in perovskite solar cells via additive engineering of the PbI2 solution. The in situ grazing incidence wide-angle X-ray scattering studies reveal that the trimethylsulfoxonium iodide (TMSOI) additive leads to an ordered solvated quasi-crystalline PbI2, which facilitates the transformation to α-phase FAPbI3 at room temperature while reacting PbI2 with FAI. As a result, the photovoltaic performance and stability of the perovskite solar cells are enhanced due to the improved optoelectronic properties of the perovskite films. A best-performing device shows a power conversion efficiency of 24.65% at one sun illumination. The unencapsulated devices stored at room temperature under 30–40% relative humidity maintain 96.40% of their initial efficiency after 1000 h.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.3c02455
Chinese Library Classification Number:
Citation Information:
In the two-step procedure for preparing a perovskite film, the chemistry of the PbI2 solution plays an important role in determining the phase stability of perovskite films. We report here sulfoxonium salt-controlled crystallization for stabilizing α-phase formamidinium lead iodide (FAPbI3) in perovskite solar cells via additive engineering of the PbI2 solution. The in situ grazing incidence wide-angle X-ray scattering studies reveal that the trimethylsulfoxonium iodide (TMSOI) additive leads to an ordered solvated quasi-crystalline PbI2, which facilitates the transformation to α-phase FAPbI3 at room temperature while reacting PbI2 with FAI. As a result, the photovoltaic performance and stability of the perovskite solar cells are enhanced due to the improved optoelectronic properties of the perovskite films. A best-performing device shows a power conversion efficiency of 24.65% at one sun illumination. The unencapsulated devices stored at room temperature under 30–40% relative humidity maintain 96.40% of their initial efficiency after 1000 h.
quote
| GB/T 7714-2015 | [1] Yalan Zhang, Tinghuan Yang, SangUk Lee, et al. ACS Energy Letters, 2024(9). DOI:10.1021/acsenergylett.3c02455. |
| MLA | [1] Yalan Zhang, et al., ACS Energy Letters, no. 9, 2024, https://doi.org/10.1021/acsenergylett.3c02455. |
| APA | [1] Yalan Zhang, Tinghuan Yang, SangUk Lee, Shengzhong Liu, Kui Zhao, & NamGyu Park. (2024). ACS Energy Letters(9). https://doi.org/10.1021/acsenergylett.3c02455 |