The Overlooked Role of Copper Surface Texture in Electrodeposition of Lithium Revealed by Electron Backscatter Diffraction AITranslate

Shanghai Jiao Tong University; Shanghai Jiao Tong University;Oxford MAG Group, Oxford Instruments Technology (Shanghai) Co. Limited; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ultrathin Cu foils play an important role in current Li-ion batteries and next-generation anode-free Li metal batteries. The surface microstructure of the Cu foil should impact the Li deposition on Cu, but a mechanistic understanding is surprisingly lacking. In this work, we employ electron backscatter diffraction to obtain statistical information on the surface texture of two archetypical ultrathin (10 μm-thick) Cu foil samples (i.e., electrodeposited Cu foil and rolled-annealed Cu foil, denoted as ED-Cu and RA-Cu). We discovered that the ED-Cu and RA-Cu foils are distinct in surface grain morphology, preferred grain orientation, and misorientation angle distribution. The front and back surfaces of the ED-Cu foil also differed in grain size and grain boundary (GB) microstructure. We further show that the grain size and the spatial distribution of the deposited Li particles can be correlated with the density of the low Σ coincidence site lattice type of GBs at the Cu surface, which plays a previously under-appreciated role in the nucleation and the subsequent growth processes of Li electrodeposition on Cu.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c02132

Chinese Library Classification Number:

Citation Information:

Ultrathin Cu foils play an important role in current Li-ion batteries and next-generation anode-free Li metal batteries. The surface microstructure of the Cu foil should impact the Li deposition on Cu, but a mechanistic understanding is surprisingly lacking. In this work, we employ electron backscatter diffraction to obtain statistical information on the surface texture of two archetypical ultrathin (10 μm-thick) Cu foil samples (i.e., electrodeposited Cu foil and rolled-annealed Cu foil, denoted as ED-Cu and RA-Cu). We discovered that the ED-Cu and RA-Cu foils are distinct in surface grain morphology, preferred grain orientation, and misorientation angle distribution. The front and back surfaces of the ED-Cu foil also differed in grain size and grain boundary (GB) microstructure. We further show that the grain size and the spatial distribution of the deposited Li particles can be correlated with the density of the low Σ coincidence site lattice type of GBs at the Cu surface, which plays a previously under-appreciated role in the nucleation and the subsequent growth processes of Li electrodeposition on Cu.

quote

GB/T 7714-2015 [1] Weina Wang, Zhiyuan Li, Shuai Chen, et al. ACS Energy Letters, 2024(9). DOI:10.1021/acsenergylett.3c02132.
MLA [1] Weina Wang, et al., ACS Energy Letters, no. 9, 2024, https://doi.org/10.1021/acsenergylett.3c02132.
APA [1] Weina Wang, Zhiyuan Li, Shuai Chen, Yong Wang, YuShi He, ZiFeng Ma, & Linsen Li. (2024). ACS Energy Letters(9). https://doi.org/10.1021/acsenergylett.3c02132
IEEE [1] Weina Wang, Zhiyuan Li, Shuai Chen, Yong Wang, YuShi He, ZiFeng Ma, and Linsen Li, ACS Energy Letters, no. 9, 2024, doi: 10.1021/acsenergylett.3c02132.