Benzotriazole-Based p-Type Polymers with Thieno[3,2-b]thiophene π-Bridges and Fluorine Substituents To Realize High VOC AITranslate

University of Chinese Academy of Sciences; Nanjing Tech University (NanjingTech); Nanjing Tech University (NanjingTech); Nanjing Tech University (NanjingTech); University of Chinese Academy of Sciences; University of Chinese Academy of Sciences;CAS Key Laboratory of Nanosystem and Hierarchical Fabrication; Zhengzhou University; Zhengzhou University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

On the basis of the success of the “Same-Acceptor-Strategy” (SAS) in constructing p-type and n-type photovoltaic material combination to realize high open-circuit voltage (VOC) beyond 1.1 V, we designed and synthesized two new benzotriazole (BTA)-based conjugated p-type polymers. PE1 was derived from the classical polymer J61 by replacing the thiophene π-bridge with thieno[3,2-b]thiophene (TT) due to its rigid structure and the linear polymer backbone conformation, which are benificial for enhancing the effective conjugation length and intermolecular π–π stacking. By further introducing fluorine atoms to the thiophene side chain in PE1, the final polymer PE2 can thus realize a downshifted highest occupied molecular orbital energy level of −5.41 eV. Utilizing SAS and adopting a benzotriazole-containing small molecule BTA3 as electron acceptor, PE1 can realize a slightly improved power conversion efficiency (PCE) of 8.43% than that of J61 (8.25%) with a Voc of 1.11 V. Furthermore, PE2:BTA3 combination can attain a extremely high Voc of 1.26 V with a moderate PCE of 5.83%, which is one of the best results for organic solar cells with Voc beyond 1.2 V. Our results indicate that the incorporation of TT π-bridge and fluorine substituents are effective to finetune the optoelectronic properties of p-type polymers to realize high VOC and PCE, which can expand the choice of material combination for SAS.

KeyWords AITranslate

sameacceptorstrategy benzotriazole πbridge fluorine organic solar cells
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00156

Chinese Library Classification Number:

Citation Information:

On the basis of the success of the “Same-Acceptor-Strategy” (SAS) in constructing p-type and n-type photovoltaic material combination to realize high open-circuit voltage (VOC) beyond 1.1 V, we designed and synthesized two new benzotriazole (BTA)-based conjugated p-type polymers. PE1 was derived from the classical polymer J61 by replacing the thiophene π-bridge with thieno[3,2-b]thiophene (TT) due to its rigid structure and the linear polymer backbone conformation, which are benificial for enhancing the effective conjugation length and intermolecular π–π stacking. By further introducing fluorine atoms to the thiophene side chain in PE1, the final polymer PE2 can thus realize a downshifted highest occupied molecular orbital energy level of −5.41 eV. Utilizing SAS and adopting a benzotriazole-containing small molecule BTA3 as electron acceptor, PE1 can realize a slightly improved power conversion efficiency (PCE) of 8.43% than that of J61 (8.25%) with a Voc of 1.11 V. Furthermore, PE2:BTA3 combination can attain a extremely high Voc of 1.26 V with a moderate PCE of 5.83%, which is one of the best results for organic solar cells with Voc beyond 1.2 V. Our results indicate that the incorporation of TT π-bridge and fluorine substituents are effective to finetune the optoelectronic properties of p-type polymers to realize high VOC and PCE, which can expand the choice of material combination for SAS.

quote

GB/T 7714-2015 [1] You Chen, Qianqian Zhang, Mengzhen Du, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00156.
MLA [1] You Chen, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00156.
APA [1] You Chen, Qianqian Zhang, Mengzhen Du, Gongqiang Li, Zijie Li, Hui Huang, Yanfang Geng, Xiaoli Zhang, & Erjun Zhou. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00156
IEEE [1] You Chen, Qianqian Zhang, Mengzhen Du, Gongqiang Li, Zijie Li, Hui Huang, Yanfang Geng, Xiaoli Zhang, and Erjun Zhou, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00156. keywords: {sameacceptorstrategy;benzotriazole;πbridge;fluorine;organic solar cells}