Ductile Polyimide/Reduced Graphene Oxide Nanohybrid Films with Porous Structure Fabricated by a Green Hydrogel Strategy AITranslate

Shanghai Jiao Tong University; Tongji University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Tongji University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Polyimide/inorganics hybrid films fabricated by conventional approaches, including an in situ polymerization method, the sol–gel process, and a solution blending method, have a dramatic drop in malleability. In this work, a hydrogel strategy for preparing ductile polyimide/reduced graphene oxide (PI/rGO) nanohybrid films with internal porous structures has been proposed. The hydrogel strategy involved two steps. The polyamide acid carboxylate/GO (PAAC/GO) films were first prepared by tape casting, followed by a gelation process of the PAAC/GO aqueous solution; the PI/rGO films were then obtained after an imidization reaction of the PAAC/GO films. Interestingly, in this strategy, the PAA chains tended to self-assemble into microdomain crystalline structures assisted by their interactions with water, as revealed by XRD and Raman spectroscopy. The present PI/rGO films display more uniform microstructures, without aggregation of the rGO nanosheets. Furthermore, they exhibited an enhanced toughness property, with a high elongation at break of 37–55%. In addition, their dielectric property is more stable and less frequency-dependent due to the internal porous structure. This hydrogel strategy would appear to be a promising candidate for fabricating hybrid PI–inorganic composite materials, even other hybrid organic/inorganic composite materials with specific features.

KeyWords AITranslate

polyimide GO hydrogel organic−inorganic composite hybrid film
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00234

Chinese Library Classification Number:

Citation Information:

Polyimide/inorganics hybrid films fabricated by conventional approaches, including an in situ polymerization method, the sol–gel process, and a solution blending method, have a dramatic drop in malleability. In this work, a hydrogel strategy for preparing ductile polyimide/reduced graphene oxide (PI/rGO) nanohybrid films with internal porous structures has been proposed. The hydrogel strategy involved two steps. The polyamide acid carboxylate/GO (PAAC/GO) films were first prepared by tape casting, followed by a gelation process of the PAAC/GO aqueous solution; the PI/rGO films were then obtained after an imidization reaction of the PAAC/GO films. Interestingly, in this strategy, the PAA chains tended to self-assemble into microdomain crystalline structures assisted by their interactions with water, as revealed by XRD and Raman spectroscopy. The present PI/rGO films display more uniform microstructures, without aggregation of the rGO nanosheets. Furthermore, they exhibited an enhanced toughness property, with a high elongation at break of 37–55%. In addition, their dielectric property is more stable and less frequency-dependent due to the internal porous structure. This hydrogel strategy would appear to be a promising candidate for fabricating hybrid PI–inorganic composite materials, even other hybrid organic/inorganic composite materials with specific features.

quote

GB/T 7714-2015 [1] Zhao Chen, Faqin Tong, Dandan Zhu, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00234.
MLA [1] Zhao Chen, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00234.
APA [1] Zhao Chen, Faqin Tong, Dandan Zhu, Xuemin Lu, & Qinghua Lu. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00234
IEEE [1] Zhao Chen, Faqin Tong, Dandan Zhu, Xuemin Lu, and Qinghua Lu, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00234. keywords: {polyimide;GO;hydrogel;organic−inorganic composite;hybrid film}