Tri-Layer Nonwoven Separator with Thermal Shutdown Function Fabricated through a Facile Papermaking Method for High-Safety Lithium-Ion Battery AITranslate

South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Lithium-ion batteries have long been plagued by the safety issue of thermal runaway. Improving the thermal stability and developing the thermal shutdown function of the separators are considered reliable solutions. Therefore, in this work, a tri-layer structured nonwoven separator with a thermal shutdown function has been prepared via the papermaking method. The separator comprises a polyethylene fiber layer, a microfibrillated cellulose fibers layer, and a polyethylene terephthalate nonwoven fabric layer. The polyethylene fiber layer endows the separator with a thermal shutdown function at 135 °C. The middle polyethylene terephthalate nonwoven layer provides support, while the microfibrillated cellulose fibers adjust the pore size. The separators exhibit excellent thermal stability, no shrinkage after heat treatment at 200 °C, and a wide thermal shutdown temperature window, thereby enhancing battery safety. This research provides an approach to fabricating high-safety thermal shutdown separators.

KeyWords AITranslate

polyolefin synthetic pulp separator thermal shutdown nonwoven lithiumion battery
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00709

Chinese Library Classification Number:

Citation Information:

Lithium-ion batteries have long been plagued by the safety issue of thermal runaway. Improving the thermal stability and developing the thermal shutdown function of the separators are considered reliable solutions. Therefore, in this work, a tri-layer structured nonwoven separator with a thermal shutdown function has been prepared via the papermaking method. The separator comprises a polyethylene fiber layer, a microfibrillated cellulose fibers layer, and a polyethylene terephthalate nonwoven fabric layer. The polyethylene fiber layer endows the separator with a thermal shutdown function at 135 °C. The middle polyethylene terephthalate nonwoven layer provides support, while the microfibrillated cellulose fibers adjust the pore size. The separators exhibit excellent thermal stability, no shrinkage after heat treatment at 200 °C, and a wide thermal shutdown temperature window, thereby enhancing battery safety. This research provides an approach to fabricating high-safety thermal shutdown separators.

quote

GB/T 7714-2015 [1] Yao Li, Jin Long, Yun Liang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00709.
MLA [1] Yao Li, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00709.
APA [1] Yao Li, Jin Long, Yun Liang, & Jian Hu. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00709
IEEE [1] Yao Li, Jin Long, Yun Liang, and Jian Hu, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00709. keywords: {polyolefin synthetic pulp;separator;thermal shutdown;nonwoven;lithiumion battery}