An efficient method for multiscale modelling of the mechanical properties of additively manufactured parts with site-specific microstructures AITranslate

Nanyang Technological University; Nanyang Technological University; Nanyang Technological University; Nanyang Technological University;HP Labs, 1501 Page Mill Rd.; Nanyang Technological University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The ability to modulate microstructures at different locations within a part (i.e., site-specific microstructures) can lead to tailored properties and enhanced performance. However, it remains challenging to efficiently model the mechanical response of such materials due to the need for extensive multiscale analysis. To address this issue, we demonstrate through microstructure-based finite element simulations, that the mechanical properties of a randomly distributed two-phase microstructure are primarily dependent on the phase fraction. Therefore, by establishing a mathematical relationship between the phase fraction and mechanical properties, the local material properties can be efficiently calculated from the local microstructure. Later, these site-specific properties were incorporated into a finite element structure to predict the global mechanical properties of the sample part. To validate the effectiveness of the proposed method, low alloy steel with site-specific microstructures was fabricated using binder jet additive manufacturing by depositing varying concentrations of carbon binder at different locations inside the part. We observed a strong agreement between the experimental and simulation stress-strain responses of the steel samples. This method can potentially pave the way for the development of a non-destructive qualification method for additively manufactured parts, as well as provide an efficient approach to multiscale modeling of material behavior, which may help accelerate the design and innovation of novel material systems. Graphical Download : Download high-res image (272KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.addma.2024.103995

Chinese Library Classification Number:

Citation Information:

The ability to modulate microstructures at different locations within a part (i.e., site-specific microstructures) can lead to tailored properties and enhanced performance. However, it remains challenging to efficiently model the mechanical response of such materials due to the need for extensive multiscale analysis. To address this issue, we demonstrate through microstructure-based finite element simulations, that the mechanical properties of a randomly distributed two-phase microstructure are primarily dependent on the phase fraction. Therefore, by establishing a mathematical relationship between the phase fraction and mechanical properties, the local material properties can be efficiently calculated from the local microstructure. Later, these site-specific properties were incorporated into a finite element structure to predict the global mechanical properties of the sample part. To validate the effectiveness of the proposed method, low alloy steel with site-specific microstructures was fabricated using binder jet additive manufacturing by depositing varying concentrations of carbon binder at different locations inside the part. We observed a strong agreement between the experimental and simulation stress-strain responses of the steel samples. This method can potentially pave the way for the development of a non-destructive qualification method for additively manufactured parts, as well as provide an efficient approach to multiscale modeling of material behavior, which may help accelerate the design and innovation of novel material systems. Graphical Download : Download high-res image (272KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Li Sun, PoJu Chiang, Jonathan Jeevan Singham, et al. Additive Manufacturing, 2024(81). DOI:10.1016/j.addma.2024.103995.
MLA [1] Li Sun, et al., Additive Manufacturing, no. 81, 2024, https://doi.org/10.1016/j.addma.2024.103995.
APA [1] Li Sun, PoJu Chiang, Jonathan Jeevan Singham, Wei Xin Tan, John Samuel Dilip Jangam, & Chang Quan Lai. (2024). Additive Manufacturing(81). https://doi.org/10.1016/j.addma.2024.103995
IEEE [1] Li Sun, PoJu Chiang, Jonathan Jeevan Singham, Wei Xin Tan, John Samuel Dilip Jangam, and Chang Quan Lai, Additive Manufacturing, no. 81, 2024, doi: 10.1016/j.addma.2024.103995.