Moisture-Induced Ionovoltaic Electricity Generation by Manipulating Organic–Inorganic Hybrid Halide Perovskites AITranslate

Indian Institute of Technology Bombay; Indian Institute of Technology Bombay; Indian Institute of Technology Bombay; Indian Institute of Technology Bombay; Indian Institute of Technology Bombay
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Attempts to satisfy the vast demands for electric power in our daily lives and to address the depletion of existing fossil fuels have led to the development of new energy conversion technologies. Herein, we present a different type of electric generation, called ionovoltaic electricity generation (IEG), that results from manipulating organic–inorganic hybrid halide perovskite structures with moisture. This IEG can generate an open-circuit voltage of up to ∼0.5 V and a short-circuit current density of ∼0.1 mA cm–2, which is sufficient to power small electronic devices. In this work we have utilized the transformation of structurally zero-dimensional perovskite, specifically MA4PbBr6·2H2O, to three-dimensional MAPbBr3 in the presence of humidity. Flexible power supply devices made of organic–inorganic hybrid perovskite layers are designed and fabricated for harvesting the energy from human breath and some other real-life conditions. This work opens a new direction in the field of organic–inorganic hybrid halide perovskites and offers an extremely simple method for energy conversion of practical importance.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00023

Chinese Library Classification Number:

Citation Information:

Attempts to satisfy the vast demands for electric power in our daily lives and to address the depletion of existing fossil fuels have led to the development of new energy conversion technologies. Herein, we present a different type of electric generation, called ionovoltaic electricity generation (IEG), that results from manipulating organic–inorganic hybrid halide perovskite structures with moisture. This IEG can generate an open-circuit voltage of up to ∼0.5 V and a short-circuit current density of ∼0.1 mA cm–2, which is sufficient to power small electronic devices. In this work we have utilized the transformation of structurally zero-dimensional perovskite, specifically MA4PbBr6·2H2O, to three-dimensional MAPbBr3 in the presence of humidity. Flexible power supply devices made of organic–inorganic hybrid perovskite layers are designed and fabricated for harvesting the energy from human breath and some other real-life conditions. This work opens a new direction in the field of organic–inorganic hybrid halide perovskites and offers an extremely simple method for energy conversion of practical importance.

quote

GB/T 7714-2015 [1] Sumit Kumar Sharma, Monika Salesh, Mohan Raj Subramaniam, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00023.
MLA [1] Sumit Kumar Sharma, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00023.
APA [1] Sumit Kumar Sharma, Monika Salesh, Mohan Raj Subramaniam, Burhanuddin Attarwala, & Aswani Yella. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00023
IEEE [1] Sumit Kumar Sharma, Monika Salesh, Mohan Raj Subramaniam, Burhanuddin Attarwala, and Aswani Yella, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00023.