daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Nanographene Coupled with Interfacial Pyrene Derivatives for Thermally Stable Perovskite Solar Cells AITranslate

Sungkyunkwan University;CY Cergy Paris Université; Sungkyunkwan University;CY Cergy Paris Université; University of Colorado Boulder; National Renewable Energy Laboratory;CY Cergy Paris Université; Sungkyunkwan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Although high-efficiency perovskite solar cells (PSCs) have been achieved using a hole-extracting material, spiro-MeOTAD, thermal stability has been unattainable due to the low glass transition temperature of spiro-MeOTAD and additives therein. Here, we report on the use of nanographene-based hole-transporting materials coupled with a pyrene derivative as an interface modifier for thermally stable and high efficiency PSCs. Asymmetric methyl and methoxy groups are introduced in the diphenylamino group that is attached to the hexa-peri-hexabenzocoronene (HBC) nanographene core, coded HBC-DPAMeOMe. 1-Pyrenemethylammonium iodide is coupled to enhance the chemical interaction between perovskite and HBC-DPAMeOMe, which leads to a power conversion efficiency over 23%. A thermal stability test at 85 °C for 1000 h reveals that 83.6% of the initial efficiency (23.04% → 19.25%) is maintained for the device with HBC-DPAMeOMe, while a significant degradation from 20.69% to 5.08% is observed for the device with spiro-MeOTAD. Nanographene-based hole conductors shed light on the thermal stability issue in PSCs.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00262

Chinese Library Classification Number:

Citation Information:

Although high-efficiency perovskite solar cells (PSCs) have been achieved using a hole-extracting material, spiro-MeOTAD, thermal stability has been unattainable due to the low glass transition temperature of spiro-MeOTAD and additives therein. Here, we report on the use of nanographene-based hole-transporting materials coupled with a pyrene derivative as an interface modifier for thermally stable and high efficiency PSCs. Asymmetric methyl and methoxy groups are introduced in the diphenylamino group that is attached to the hexa-peri-hexabenzocoronene (HBC) nanographene core, coded HBC-DPAMeOMe. 1-Pyrenemethylammonium iodide is coupled to enhance the chemical interaction between perovskite and HBC-DPAMeOMe, which leads to a power conversion efficiency over 23%. A thermal stability test at 85 °C for 1000 h reveals that 83.6% of the initial efficiency (23.04% → 19.25%) is maintained for the device with HBC-DPAMeOMe, while a significant degradation from 20.69% to 5.08% is observed for the device with spiro-MeOTAD. Nanographene-based hole conductors shed light on the thermal stability issue in PSCs.

quote

GB/T 7714-2015 [1] SeulGi Kim, Thybault de Monfreid, JeongHyeon Kim, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00262.
MLA [1] SeulGi Kim, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00262.
APA [1] SeulGi Kim, Thybault de Monfreid, JeongHyeon Kim, Fabrice Goubard, Joseph J. Berry, Kai Zhu, ThanhTuân Bui, & NamGyu Park. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00262
IEEE [1] SeulGi Kim, Thybault de Monfreid, JeongHyeon Kim, Fabrice Goubard, Joseph J. Berry, Kai Zhu, ThanhTuân Bui, and NamGyu Park, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00262.