Abstract AITranslate

Compared with inorganic photovoltaics, organic photovoltaics (OPVs) still have a low fill factor (FF) that restricts their power conversion efficiency (PCE). The FF is determined by the resistances that are influenced by carriers recombination. In this work, the tandem structure is demonstrated to be a feasible solution to improve the FF of OPVs. The recombination losses of subcells in the tandem structure are reduced and consequently improves the FF. When the two subcells are stacked in a tandem structure, the highest value of the FF reaches 76.6%, much higher than that of 66.1% achieved by its single junction device. Finally, a PCE of 14.1% with a FF of 73.6% is achieved in a tandem OPV after optimizing the thickness of each active layer. This work not only demonstrates the inherent mechanism for a higher FF in tandem OPVs but also presents a feasible solution for high-performance photovoltaic devices.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b00896

Chinese Library Classification Number:

Citation Information:

Compared with inorganic photovoltaics, organic photovoltaics (OPVs) still have a low fill factor (FF) that restricts their power conversion efficiency (PCE). The FF is determined by the resistances that are influenced by carriers recombination. In this work, the tandem structure is demonstrated to be a feasible solution to improve the FF of OPVs. The recombination losses of subcells in the tandem structure are reduced and consequently improves the FF. When the two subcells are stacked in a tandem structure, the highest value of the FF reaches 76.6%, much higher than that of 66.1% achieved by its single junction device. Finally, a PCE of 14.1% with a FF of 73.6% is achieved in a tandem OPV after optimizing the thickness of each active layer. This work not only demonstrates the inherent mechanism for a higher FF in tandem OPVs but also presents a feasible solution for high-performance photovoltaic devices.

quote

GB/T 7714-2015 [1] Yuqiang Liu, Pei Cheng, Jun Yuan, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00896.
MLA [1] Yuqiang Liu, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00896.
APA [1] Yuqiang Liu, Pei Cheng, Jun Yuan, Tianyi Huang, Rui Wang, Dong Meng, Bineh Ndefru, Yingping Zou, Baoquan Sun, & Yang Yang. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00896
IEEE [1] Yuqiang Liu, Pei Cheng, Jun Yuan, Tianyi Huang, Rui Wang, Dong Meng, Bineh Ndefru, Yingping Zou, Baoquan Sun, and Yang Yang, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00896.