daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Stable Unassisted Solar Water Splitting on Semiconductor Photocathodes Protected by Multifunctional GaN Nanostructures AITranslate

University of Michigan; University of Michigan; University of Michigan; University of Michigan; University of Michigan
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Producing hydrogen by unassisted solar water splitting is one essential step to make direct solar fuel conversion a viable energy source. To date, however, there has been no demonstration of stable photoelectrodes for high-efficiency photoelectrochemical water splitting. In this work, we report that a GaInP2/GaAs/Ge triple-junction (3J) photocathode protected by multifunctional GaN nanostructures can enable both efficient and relatively stable solar water splitting. A 12.6% solar-to-hydrogen (STH) efficiency is measured without any external bias. Of particular importance, we demonstrate relatively stable solar water splitting for 80 h in three-electrode configuration and 57 h in two-electrode measurement at zero bias. This is the best reported stability for multijunction III-V semiconductor photocathodes in two-electrode configuration to our knowledge. The multifunctional GaN nanostructure significantly reduces the charge transfer resistance at the semiconductor/electrolyte interface and protects III–V materials against corrosion. Such multifunctional GaN photocatalytic nanostructures provide a new pathway to improve the performance of conventional photoelectrodes to achieve both efficient and stable unassisted solar water splitting.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b00549

Chinese Library Classification Number:

Citation Information:

Producing hydrogen by unassisted solar water splitting is one essential step to make direct solar fuel conversion a viable energy source. To date, however, there has been no demonstration of stable photoelectrodes for high-efficiency photoelectrochemical water splitting. In this work, we report that a GaInP2/GaAs/Ge triple-junction (3J) photocathode protected by multifunctional GaN nanostructures can enable both efficient and relatively stable solar water splitting. A 12.6% solar-to-hydrogen (STH) efficiency is measured without any external bias. Of particular importance, we demonstrate relatively stable solar water splitting for 80 h in three-electrode configuration and 57 h in two-electrode measurement at zero bias. This is the best reported stability for multijunction III-V semiconductor photocathodes in two-electrode configuration to our knowledge. The multifunctional GaN nanostructure significantly reduces the charge transfer resistance at the semiconductor/electrolyte interface and protects III–V materials against corrosion. Such multifunctional GaN photocatalytic nanostructures provide a new pathway to improve the performance of conventional photoelectrodes to achieve both efficient and stable unassisted solar water splitting.

quote

GB/T 7714-2015 [1] Yongjie Wang, Jonathan Schwartz, Jiseok Gim, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00549.
MLA [1] Yongjie Wang, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00549.
APA [1] Yongjie Wang, Jonathan Schwartz, Jiseok Gim, Robert Hovden, & Zetian Mi. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00549
IEEE [1] Yongjie Wang, Jonathan Schwartz, Jiseok Gim, Robert Hovden, and Zetian Mi, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00549.