Flame retardants (FR) are inevitable additives to many plastics. Halogenated organics are effective FRs but are controversially discussed due to the release of toxic gases during a fire or their persistence if landfilled. Phosphorus-containing compounds are effective alternatives to halogenated FRs and have potential lower toxicity and degradability. In addition, nitrogen-containing additives were reported to induce synergistic effects with phosphorus-based FRs. However, no systematic study of the gradual variation on a single phosphorus FR containing both P–O and P–N moieties and their comparison to the respective blends of phosphates and phosphoramides was reported. This study developed general design principles for P–O- and P–N-based FRs and will help to design effective FRs for various polymers. We synthesized a library of phosphorus FRs that only differ in their P-binding pattern from each other and studied their decomposition mechanism in epoxy resins. Systematic control over the decomposition pathways of phosphate (P═O(OR)3), phosphoramidate (P═O(OR)2(NHR)), phosphorodiamidate (P═O(OR)(NHR)2), phosphoramide (P═O(NHR)3), and their blends was identified, for example, by reducing cis-elimination and the formation of P–N-rich char with increasing nitrogen content in the P-binding sphere. Our FR epoxy resins can compete with commercial FRs in most cases, but we proved that the blending of esters and amides outperformed the single-molecule amidates/diamidates due to distinctively different decomposition mechanisms acting synergistically when blended.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.9b00129
Chinese Library Classification Number:
Citation Information:
Flame retardants (FR) are inevitable additives to many plastics. Halogenated organics are effective FRs but are controversially discussed due to the release of toxic gases during a fire or their persistence if landfilled. Phosphorus-containing compounds are effective alternatives to halogenated FRs and have potential lower toxicity and degradability. In addition, nitrogen-containing additives were reported to induce synergistic effects with phosphorus-based FRs. However, no systematic study of the gradual variation on a single phosphorus FR containing both P–O and P–N moieties and their comparison to the respective blends of phosphates and phosphoramides was reported. This study developed general design principles for P–O- and P–N-based FRs and will help to design effective FRs for various polymers. We synthesized a library of phosphorus FRs that only differ in their P-binding pattern from each other and studied their decomposition mechanism in epoxy resins. Systematic control over the decomposition pathways of phosphate (P═O(OR)3), phosphoramidate (P═O(OR)2(NHR)), phosphorodiamidate (P═O(OR)(NHR)2), phosphoramide (P═O(NHR)3), and their blends was identified, for example, by reducing cis-elimination and the formation of P–N-rich char with increasing nitrogen content in the P-binding sphere. Our FR epoxy resins can compete with commercial FRs in most cases, but we proved that the blending of esters and amides outperformed the single-molecule amidates/diamidates due to distinctively different decomposition mechanisms acting synergistically when blended.
quote
| GB/T 7714-2015 | [1] Jens C. Markwart, Alexander Battig, Lisa Zimmermann, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00129. |
| MLA | [1] Jens C. Markwart, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00129. |
| APA | [1] Jens C. Markwart, Alexander Battig, Lisa Zimmermann, Martin Wagner, Jochen Fischer, Bernhard Schartel, & Frederik R. Wurm. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00129 |
| IEEE | [1] Jens C. Markwart, Alexander Battig, Lisa Zimmermann, Martin Wagner, Jochen Fischer, Bernhard Schartel, and Frederik R. Wurm, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00129. keywords: {phosphorus;flame retardants;epoxies;mechanistic study;toxicity} |