This work reports several 1,5-diaminoanthraquinone (1,5-DAAQ)-based visible-light-sensitive photoinitiating systems (PISs), which can efficiently initiate the free radical photopolymerization of (meth)acrylates under green light delivered from light-emitting diode. The PISs contain three components: 1,5-diaminoanthraquinone, an iodonium salt, and aromatic amines. In one example, polymerization could be efficiently initiated and completed within 10 s with double bond conversions of approximately 80%. The initiating system could also be used in conjunction with reversible addition–fragmentation chain transfer (RAFT) polymerization. Finally, the 1,5-DAAQ/iodonium salt/4-N,N-trimethylaniline PIS could be readily employed in the 3D printing process of polymer/carbon nanotube nanocomposites.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.9b00140
Chinese Library Classification Number:
Citation Information:
This work reports several 1,5-diaminoanthraquinone (1,5-DAAQ)-based visible-light-sensitive photoinitiating systems (PISs), which can efficiently initiate the free radical photopolymerization of (meth)acrylates under green light delivered from light-emitting diode. The PISs contain three components: 1,5-diaminoanthraquinone, an iodonium salt, and aromatic amines. In one example, polymerization could be efficiently initiated and completed within 10 s with double bond conversions of approximately 80%. The initiating system could also be used in conjunction with reversible addition–fragmentation chain transfer (RAFT) polymerization. Finally, the 1,5-DAAQ/iodonium salt/4-N,N-trimethylaniline PIS could be readily employed in the 3D printing process of polymer/carbon nanotube nanocomposites.
quote
| GB/T 7714-2015 | [1] Guannan Wang, Nicholas S. Hill, Di Zhu, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00140. |
| MLA | [1] Guannan Wang, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00140. |
| APA | [1] Guannan Wang, Nicholas S. Hill, Di Zhu, Pu Xiao, Michelle L. Coote, & Martina H. Stenzel. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00140 |