Electric Field-Assisted Self-Assembly of Diphenylalanine Peptides for High-Performance Energy Conversion AITranslate

University of Chinese Academy of Sciences; Xidian University; Xidian University; Xidian University; Xidian University; Georgia Institute of Technology; Xidian University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Peptide-based piezoelectric materials have emerged as a new class of intelligent biomaterials, and applying electric fields during growth was found to result in uniform polarization. Here, we explore in-depth the effect of electric fields on diphenylalanine peptide crystallization and epitaxial growth. The percentage of crystals with negative polarization is linearly proportional to the electric field strength, while the trend is slightly different when a positive electric field is applied. The minimum electric field strength needed to achieve peptides with a uniform polarization is about 200 kV/m. Due to the improved crystallinity and uniform polarization in peptides, the piezoelectric constant d33 increases linearly with the applied electric fields. The output voltage and current of peptide-based piezoelectric nanogenerators increase with the applied force on the device and with the electric field used for growth material, and the power density reaches 9.98 W/m3. Our work provides direct insight into the peptide self-assembly process under electric fields and guides the fabrication of high-performance materials for degradable energy devices.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00664

Chinese Library Classification Number:

Citation Information:

Peptide-based piezoelectric materials have emerged as a new class of intelligent biomaterials, and applying electric fields during growth was found to result in uniform polarization. Here, we explore in-depth the effect of electric fields on diphenylalanine peptide crystallization and epitaxial growth. The percentage of crystals with negative polarization is linearly proportional to the electric field strength, while the trend is slightly different when a positive electric field is applied. The minimum electric field strength needed to achieve peptides with a uniform polarization is about 200 kV/m. Due to the improved crystallinity and uniform polarization in peptides, the piezoelectric constant d33 increases linearly with the applied electric fields. The output voltage and current of peptide-based piezoelectric nanogenerators increase with the applied force on the device and with the electric field used for growth material, and the power density reaches 9.98 W/m3. Our work provides direct insight into the peptide self-assembly process under electric fields and guides the fabrication of high-performance materials for degradable energy devices.

quote

GB/T 7714-2015 [1] Yusen Su, Jing Liu, Dingyi Yang, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00664.
MLA [1] Yusen Su, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00664.
APA [1] Yusen Su, Jing Liu, Dingyi Yang, Wen Hu, Xue Jiang, Zhong Lin Wang, & Rusen Yang. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00664
IEEE [1] Yusen Su, Jing Liu, Dingyi Yang, Wen Hu, Xue Jiang, Zhong Lin Wang, and Rusen Yang, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00664.