Graphene Oxide Nanosheets Induce Mitochondrial Fragmentation by Cutting through Membrane AITranslate

Shandong First Medical University & Shandong Academy of Medical Sciences; Zhejiang University; Southwest Medical University; The First Affiliated Hospital of Anhui Medical University; University of Chinese Academy of Sciences; University of Cincinnati College of Medicine; Shandong First Medical University & Shandong Academy of Medical Sciences; University of Cincinnati College of Medicine; Shandong First Medical University & Shandong Academy of Medical Sciences; The First Affiliated Hospital of Anhui Medical University; Zhejiang University; Zhejiang University; Shandong First Medical University & Shandong Academy of Medical Sciences; University of Cincinnati College of Medicine
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Graphene oxide (GO)-based nanomaterials have unique physical, chemical, and biological properties that make their use in biomedical research and nanomedicine of enormous interest. However, little is known about their sublethal effects on biological systems, especially mitochondrial damage. Here, by using super-resolution imaging in live cells, we discovered that GO nanosheets damage mitochondrial membranes in a dose-dependent manner in both cancer and healthy cell lines. Furthermore, we observed that GO nanosheets destroy the integrity of mitochondrial cristae. We performed simulations to clarify the mechanisms governing that behavior and found that GO nanosheets insert into membranes, thereby resulting in membrane “cutting” and that the size of GO nanosheets is an essential factor of inducing fragmentation. Those results, demonstrating that large GO nanosheets induce mitochondrial damage, indicate that the assessment and safety profiling of GO-based biomedical research tools and products should include the careful evaluation of their effects on mitochondria.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00177

Chinese Library Classification Number:

Citation Information:

Graphene oxide (GO)-based nanomaterials have unique physical, chemical, and biological properties that make their use in biomedical research and nanomedicine of enormous interest. However, little is known about their sublethal effects on biological systems, especially mitochondrial damage. Here, by using super-resolution imaging in live cells, we discovered that GO nanosheets damage mitochondrial membranes in a dose-dependent manner in both cancer and healthy cell lines. Furthermore, we observed that GO nanosheets destroy the integrity of mitochondrial cristae. We performed simulations to clarify the mechanisms governing that behavior and found that GO nanosheets insert into membranes, thereby resulting in membrane “cutting” and that the size of GO nanosheets is an essential factor of inducing fragmentation. Those results, demonstrating that large GO nanosheets induce mitochondrial damage, indicate that the assessment and safety profiling of GO-based biomedical research tools and products should include the careful evaluation of their effects on mitochondria.

quote

GB/T 7714-2015 [1] Xintian Shao, Zhou Fang, Miaoling Li, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00177.
MLA [1] Xintian Shao, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00177.
APA [1] Xintian Shao, Zhou Fang, Miaoling Li, Weiwei Zou, Qianchun Wang, Chengying Zhang, Yongchun Wei, Zhiqi Tian, Yongchao Lai, Yunxia Cao, Baohua Ji, Dechang Li, Qixin Chen, & Jiajie Diao. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00177
IEEE [1] Xintian Shao, Zhou Fang, Miaoling Li, Weiwei Zou, Qianchun Wang, Chengying Zhang, Yongchun Wei, Zhiqi Tian, Yongchao Lai, Yunxia Cao, Baohua Ji, Dechang Li, Qixin Chen, and Jiajie Diao, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00177.