Deformation processes of additively manufactured interstitial-strengthened high entropy alloy: In-situ high-energy synchrotron X-ray diffraction and microstructural appraisal AITranslate

University of Groningen; Universidade NOVA de Lisboa; Universidade NOVA de Lisboa; University of Groningen; University of Science and Technology Beijing;Institute of Materials Physics; University of Groningen; University of Groningen
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Additively manufactured components often exhibit pronounced anisotropy due to the heterogeneous microstructure generated by the complex and repetitive thermal cycling history. Grain orientation is one of the determinant microstructural features that influences the activation of different deformation mechanisms. In this work, laser powder-bed fusion (LPBF) was applied to fabricate Fe49.5Mn30Co10Cr10C0.5 interstitial-strengthened high entropy alloy (iHEA). Fabrication was performed at angles of 0° and 90° relative to the main laser scanning direction, and the plastic deformation behavior of these two oriented specimens was studied. The initial microstructure of the LPBF-built iHEA was composed of a complex heterogeneous columnar grains containing high-density dislocation network and a large number of stacking faults, as well as nano-precipitates and elemental segregation of Mn at subgrain boundaries. During uniaxial tension in-situ high-energy synchrotron X-ray diffraction (HE-SXRD) was performed to track the deformation processes and mechanisms of this metastable iHEA. The influence of different deformation mechanisms on the mechanical responses of the current LPBF-built iHEA was scrutinized combining in-situ HE-SXRD with electron backscattered diffraction (EBSD) and transmission electron microscopy (TEM) analyses, which not only gives insights into the macrostructural evolution but also provides comprehensive characterization on microstructural responses and the orientation-dependent effects imposed by the fabrication constraints originally imposed. The implemented multiscale characterization revealed the presence of a strain-induced fcc to hcp phase transformation, which is influenced by the growth texture close to <110> along the building direction. Moreover, EBSD and TEM analysis of the fracture regions uncovered the formation of nanosized deformation twins, confirming the simultaneous activation of phase transformation- and twinning-induced plasticity (TRIP and TWIP) effects. The results obtained in this work gain new insights into orientation-dependent deformation behavior of additively manufactured iHEA, which facilitates the microstructural design when exploiting the TRIP/TWIP effects. Graphical Download : Download high-res image (366KB) Download : Download full-size image

KeyWords AITranslate

Laser powderbed fusion Interstitialstrengthened high entropy alloy Insitu highenergy synchrotron Xray diffraction Deformation mechanisms Grain orientation Phase transformation Nanotwinning
No data

Basic Information:

DOI:https://doi.org/10.1016/j.addma.2023.103791

Chinese Library Classification Number:

Citation Information:

Additively manufactured components often exhibit pronounced anisotropy due to the heterogeneous microstructure generated by the complex and repetitive thermal cycling history. Grain orientation is one of the determinant microstructural features that influences the activation of different deformation mechanisms. In this work, laser powder-bed fusion (LPBF) was applied to fabricate Fe49.5Mn30Co10Cr10C0.5 interstitial-strengthened high entropy alloy (iHEA). Fabrication was performed at angles of 0° and 90° relative to the main laser scanning direction, and the plastic deformation behavior of these two oriented specimens was studied. The initial microstructure of the LPBF-built iHEA was composed of a complex heterogeneous columnar grains containing high-density dislocation network and a large number of stacking faults, as well as nano-precipitates and elemental segregation of Mn at subgrain boundaries. During uniaxial tension in-situ high-energy synchrotron X-ray diffraction (HE-SXRD) was performed to track the deformation processes and mechanisms of this metastable iHEA. The influence of different deformation mechanisms on the mechanical responses of the current LPBF-built iHEA was scrutinized combining in-situ HE-SXRD with electron backscattered diffraction (EBSD) and transmission electron microscopy (TEM) analyses, which not only gives insights into the macrostructural evolution but also provides comprehensive characterization on microstructural responses and the orientation-dependent effects imposed by the fabrication constraints originally imposed. The implemented multiscale characterization revealed the presence of a strain-induced fcc to hcp phase transformation, which is influenced by the growth texture close to <110> along the building direction. Moreover, EBSD and TEM analysis of the fracture regions uncovered the formation of nanosized deformation twins, confirming the simultaneous activation of phase transformation- and twinning-induced plasticity (TRIP and TWIP) effects. The results obtained in this work gain new insights into orientation-dependent deformation behavior of additively manufactured iHEA, which facilitates the microstructural design when exploiting the TRIP/TWIP effects. Graphical Download : Download high-res image (366KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Wei Zhang, Jiajia Shen, J.P. Oliveira, et al. Additive Manufacturing, 2023(76). DOI:10.1016/j.addma.2023.103791.
MLA [1] Wei Zhang, et al., Additive Manufacturing, no. 76, 2023, https://doi.org/10.1016/j.addma.2023.103791.
APA [1] Wei Zhang, Jiajia Shen, J.P. Oliveira, Hui Wang, Shaochuan Feng, N. Schell, Bart J. Kooi, & Yutao Pei. (2023). Additive Manufacturing(76). https://doi.org/10.1016/j.addma.2023.103791
IEEE [1] Wei Zhang, Jiajia Shen, J.P. Oliveira, Hui Wang, Shaochuan Feng, N. Schell, Bart J. Kooi, and Yutao Pei, Additive Manufacturing, no. 76, 2023, doi: 10.1016/j.addma.2023.103791. keywords: {Laser powderbed fusion;Interstitialstrengthened high entropy alloy;Insitu highenergy synchrotron Xray diffraction;Deformation mechanisms;Grain orientation;Phase transformation;Nanotwinning}