daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Dithienobenzothiadiazole-Bridged Nonfullerene Electron Acceptors for Efficient Organic Solar Cells AITranslate

South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Advances of small-molecular acceptors (SMAs) recently have motivated the development of high-performance organic solar cells (OSCs). The SMAs featuring A–D–C–D–A framework have attracted numerous attention due to their facile tunability on chemical structures and in commercial synthesis. In this work, dithienobenzothiadiazol (DTBT) was utilized as the center (C) unit of A–D–C–D–A SMAs and three corresponding SMAs named DTBCIC-Cl, DTBCIC-F, and DTBCIC-H were synthesized by altering the terminal groups. The variation of terminal groups endowed SMAs with different performances, including optical absorbance, energy levels, and molecular packing, etc. In comparison to DTBCIC-H, DTBCIC-Cl and DTBCIC-F obtained by halogenation showed red-shift absorption, well matched energy levels with the polymer donor PM6, as well as closer molecular packing, rendering the blend films based on PM6:DTBCIC-Cl and PM6:DTBCIC-F wide absorption and improved morphology. High power conversion efficiency of 12.71% was thus obtained for OSCs based on DTBCIC-Cl. The results prove that optimization of SMAs via altering terminal groups provides a promising design strategy to obtain high-performance A–D–C–D–A SMAs.

KeyWords AITranslate

organic solar cells dithienobenzothiadiazol A−D−C−D−A framework smallmolecule acceptors nonfullerene acceptors
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01406

Chinese Library Classification Number:

Citation Information:

Advances of small-molecular acceptors (SMAs) recently have motivated the development of high-performance organic solar cells (OSCs). The SMAs featuring A–D–C–D–A framework have attracted numerous attention due to their facile tunability on chemical structures and in commercial synthesis. In this work, dithienobenzothiadiazol (DTBT) was utilized as the center (C) unit of A–D–C–D–A SMAs and three corresponding SMAs named DTBCIC-Cl, DTBCIC-F, and DTBCIC-H were synthesized by altering the terminal groups. The variation of terminal groups endowed SMAs with different performances, including optical absorbance, energy levels, and molecular packing, etc. In comparison to DTBCIC-H, DTBCIC-Cl and DTBCIC-F obtained by halogenation showed red-shift absorption, well matched energy levels with the polymer donor PM6, as well as closer molecular packing, rendering the blend films based on PM6:DTBCIC-Cl and PM6:DTBCIC-F wide absorption and improved morphology. High power conversion efficiency of 12.71% was thus obtained for OSCs based on DTBCIC-Cl. The results prove that optimization of SMAs via altering terminal groups provides a promising design strategy to obtain high-performance A–D–C–D–A SMAs.

quote

GB/T 7714-2015 [1] Yixu Tang, Hexiang Feng, Yuanying Liang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.1c01406.
MLA [1] Yixu Tang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.1c01406.
APA [1] Yixu Tang, Hexiang Feng, Yuanying Liang, Haoran Tang, Zurong Du, Jiaxin Xu, Fei Huang, & Yong Cao. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.1c01406
IEEE [1] Yixu Tang, Hexiang Feng, Yuanying Liang, Haoran Tang, Zurong Du, Jiaxin Xu, Fei Huang, and Yong Cao, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.1c01406. keywords: {organic solar cells;dithienobenzothiadiazol;A−D−C−D−A framework;smallmolecule acceptors;nonfullerene acceptors}