daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Silicon Electrodes for Li-Ion Batteries. Addressing the Challenges through Coordination Chemistry AITranslate

Université de Nantes; Université de Nantes;Centre Énergie
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Silicon is considered as a promising negative electrode active material for Li-ion batteries, but its practical use is hampered by its very limited electrochemical cyclability arising from its major volume change upon cycling, which deteriorates the electrode architecture and the solid–electrolyte interphase. In this Perspective, we aim at critically discussing the opportunities offered by coordination chemistry to tackle these challenges. More precisely, we will show how the characteristics of the coordination bonds, notably their tunability, medium strength, and dynamic character, can be exploited to offer alternative paths for binding, templating, and coating Si particles in order to ultimately improve the cycle life of Si electrodes in Li-ion batteries.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b02433

Chinese Library Classification Number:

Citation Information:

Silicon is considered as a promising negative electrode active material for Li-ion batteries, but its practical use is hampered by its very limited electrochemical cyclability arising from its major volume change upon cycling, which deteriorates the electrode architecture and the solid–electrolyte interphase. In this Perspective, we aim at critically discussing the opportunities offered by coordination chemistry to tackle these challenges. More precisely, we will show how the characteristics of the coordination bonds, notably their tunability, medium strength, and dynamic character, can be exploited to offer alternative paths for binding, templating, and coating Si particles in order to ultimately improve the cycle life of Si electrodes in Li-ion batteries.

quote

GB/T 7714-2015 [1] Thomas Devic, Bernard Lestriez, Lionel Roué. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.8b02433.
MLA [1] Thomas Devic, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.8b02433.
APA [1] Thomas Devic, Bernard Lestriez, & Lionel Roué. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.8b02433
IEEE [1] Thomas Devic, Bernard Lestriez, and Lionel Roué, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.8b02433.