Particulate Photocatalysts for Water Splitting: Recent Advances and Future Prospects AITranslate
Abstract AITranslate
Water splitting via photocatalysis has the potential to produce clean, renewable hydrogen. Although various new photocatalysts have been reported, developing semiconductor materials that efficiently convert the energy in sunlight remains the primary challenge. This Perspective focuses on representative examples of particulate photocatalysts for overall water splitting. The design of both photocatalytic materials and overall systems intended for large-scale operation is discussed.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b02209
Chinese Library Classification Number:
Citation Information:
Water splitting via photocatalysis has the potential to produce clean, renewable hydrogen. Although various new photocatalysts have been reported, developing semiconductor materials that efficiently convert the energy in sunlight remains the primary challenge. This Perspective focuses on representative examples of particulate photocatalysts for overall water splitting. The design of both photocatalytic materials and overall systems intended for large-scale operation is discussed.
quote
| GB/T 7714-2015 | [1] Tsuyoshi Takata, Kazunari Domen. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.8b02209. |
| MLA | [1] Tsuyoshi Takata, and Kazunari Domen. ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.8b02209. |
| APA | [1] Tsuyoshi Takata, & Kazunari Domen. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.8b02209 |
| IEEE | [1] Tsuyoshi Takata and Kazunari Domen, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.8b02209. |