daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Double-Network Protein Hydrogels as Flexible Pressure Sensors for Contactless Delivery AITranslate

Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

To meet the growing demand for sustainable development and ecofriendliness, hydrogels based on biopolymers have attracted widespread attention for developing flexible pressure sensors. Natural globular proteins exhibit great potential for developing biobased pressure sensors owing to their advantages of high water solubility, easy gelation, biocompatibility, and low production cost. However, realizing globular protein hydrogel-based sensors with interfacial and bulk toughness for pressure sensing and use in wearable devices remains a challenge. This study focuses on developing a high-performance flexible pressure sensor based on a biobased protein hydrogel. Consequently, a flexible protein/polyacrylamide (PAM) hydrogel with a featured double-network (DN) structure linked covalently with hydrogen bonds was first synthesized via a one-pot method based on natural ovalbumin (OVA). The unique DN structure of the as-synthesized OVA/PAM hydrogel affords excellent mechanical performance, flexibility, and adhesion properties. The mechanical properties of the DN hydrogel were enhanced after further cross-linking with Fe3+ and treatment with glycerol. Subsequently, the flexible pressure sensor was constructed by sandwiching a microstructured OVA/PAM dielectric layer between two flexible silver nanowire electrodes. The obtained sensor exhibits a high sensitivity of 2.9 kPa–1 and a short response time of 18 ms, ensuring the ability to monitor physiological signals. Based on its excellent performance, the fabricated sensor was used for monitoring the signals obtained using practical applications such as wrist bending, finger knocking, stretching, international Morse code, and pressure distribution. Particularly, we implemented a contactless delivery system using the fabricated OVA-based pressure sensors linked to unmanned vehicles and global positioning systems, providing a solution for low-risk commodity distribution during Coronavirus disease 2019 (COVID-19).

KeyWords AITranslate

doublenetwork hydrogels contactless delivery pressure sensor protein flexible
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01696

Chinese Library Classification Number:

Citation Information:

To meet the growing demand for sustainable development and ecofriendliness, hydrogels based on biopolymers have attracted widespread attention for developing flexible pressure sensors. Natural globular proteins exhibit great potential for developing biobased pressure sensors owing to their advantages of high water solubility, easy gelation, biocompatibility, and low production cost. However, realizing globular protein hydrogel-based sensors with interfacial and bulk toughness for pressure sensing and use in wearable devices remains a challenge. This study focuses on developing a high-performance flexible pressure sensor based on a biobased protein hydrogel. Consequently, a flexible protein/polyacrylamide (PAM) hydrogel with a featured double-network (DN) structure linked covalently with hydrogen bonds was first synthesized via a one-pot method based on natural ovalbumin (OVA). The unique DN structure of the as-synthesized OVA/PAM hydrogel affords excellent mechanical performance, flexibility, and adhesion properties. The mechanical properties of the DN hydrogel were enhanced after further cross-linking with Fe3+ and treatment with glycerol. Subsequently, the flexible pressure sensor was constructed by sandwiching a microstructured OVA/PAM dielectric layer between two flexible silver nanowire electrodes. The obtained sensor exhibits a high sensitivity of 2.9 kPa–1 and a short response time of 18 ms, ensuring the ability to monitor physiological signals. Based on its excellent performance, the fabricated sensor was used for monitoring the signals obtained using practical applications such as wrist bending, finger knocking, stretching, international Morse code, and pressure distribution. Particularly, we implemented a contactless delivery system using the fabricated OVA-based pressure sensors linked to unmanned vehicles and global positioning systems, providing a solution for low-risk commodity distribution during Coronavirus disease 2019 (COVID-19).

quote

GB/T 7714-2015 [1] Anbo Zheng, Yuxiang Qin, Qing Xia, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01696.
MLA [1] Anbo Zheng, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01696.
APA [1] Anbo Zheng, Yuxiang Qin, Qing Xia, Xueshuo Zhang, & Yanxu Chen. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01696
IEEE [1] Anbo Zheng, Yuxiang Qin, Qing Xia, Xueshuo Zhang, and Yanxu Chen, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01696. keywords: {doublenetwork hydrogels;contactless delivery;pressure sensor;protein;flexible}