A Noncontact Constant-Voltage Triboelectric Nanogenerator via Charge Excitation AITranslate

Guangxi University;Beijing Institute of Nanoenergy and Nanosystems;Beijing Institute of Nanoenergy and Nanosystems;Beijing Institute of Nanoenergy and Nanosystems;Beijing Institute of Nanoenergy and Nanosystems; Beijing Jiaotong University;Beijing Institute of Nanoenergy and Nanosystems; Guangxi University;Beijing Institute of Nanoenergy and Nanosystems; P. R. China|Georgia Institute of Technology; Guangxi University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Triboelectric nanogenerators (TENGs) have attracted great attention in the distributed power sources field due to their ability to convert environment mechanical energy into electrical energy. However, the power density, durability, and humidity resistance of TENGs remain to be improved for large-scale application. Here, a noncontact constant-voltage triboelectric nanogenerator via charge excitation (ECV-TENG) is proposed to enhance the output performance, which first applies an adaptive-contact constant-voltage TENG as a charge pump and generates constant-voltage output via an elaborate noncontact phase-shift design. The ECV-TENG achieves an average power of 12.74 W m–3 Hz–2 and exhibits a long service life of over 2,000,000 cycles. Moreover, thanks to the humidity resistance of the constant-voltage pump and noncontact TENG, the ECV-TENG demonstrates a good humidity resistance at humidity up to 90%. This work not only promotes the potential applications of TENGs as a distributed energy supply but also provides new insights toward large-scale energy harvesting by TENGs.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00378

Chinese Library Classification Number:

Citation Information:

Triboelectric nanogenerators (TENGs) have attracted great attention in the distributed power sources field due to their ability to convert environment mechanical energy into electrical energy. However, the power density, durability, and humidity resistance of TENGs remain to be improved for large-scale application. Here, a noncontact constant-voltage triboelectric nanogenerator via charge excitation (ECV-TENG) is proposed to enhance the output performance, which first applies an adaptive-contact constant-voltage TENG as a charge pump and generates constant-voltage output via an elaborate noncontact phase-shift design. The ECV-TENG achieves an average power of 12.74 W m–3 Hz–2 and exhibits a long service life of over 2,000,000 cycles. Moreover, thanks to the humidity resistance of the constant-voltage pump and noncontact TENG, the ECV-TENG demonstrates a good humidity resistance at humidity up to 90%. This work not only promotes the potential applications of TENGs as a distributed energy supply but also provides new insights toward large-scale energy harvesting by TENGs.

quote

GB/T 7714-2015 [1] Yuexiao Hu, Xinyuan Li, Yikui Gao, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00378.
MLA [1] Yuexiao Hu, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00378.
APA [1] Yuexiao Hu, Xinyuan Li, Yikui Gao, Zhihao Zhao, Baofeng Zhang, Chuguo Zhang, Lixia He, Jiaqi Liu, Linglin Zhou, Zhong Lin Wang, & Jie Wang. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00378
IEEE [1] Yuexiao Hu, Xinyuan Li, Yikui Gao, Zhihao Zhao, Baofeng Zhang, Chuguo Zhang, Lixia He, Jiaqi Liu, Linglin Zhou, Zhong Lin Wang, and Jie Wang, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00378.