Reducing Open-Circuit Voltage Losses in All-Inorganic Perovskite Cells by Dedoping AITranslate

Institute of Materials for Electronics and Energy Technology (i-MEET);Institute of Materials for Electronics and Energy Technology (i-MEET);Institute of Materials for Electronics and Energy Technology (i-MEET);Institute of Materials for Electronics and Energy Technology (i-MEET);Institute of Materials for Electronics and Energy Technology (i-MEET);Institute of Materials for Electronics and Energy Technology (i-MEET);Institute of Materials for Electronics and Energy Technology (i-MEET); Jinan University; Germany|Helmholtz-Institute Erlangen-Nürnberg (HI ERN); South China University of Technology; Germany|Helmholtz-Institute Erlangen-Nürnberg (HI ERN)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

CsPbI2Br is an attractive photovoltaic material due to its promising optoelectronic properties. However, the corresponding perovskite solar cells (PSCs) with p-i-n configuration suffer from low open-circuit voltage (VOC) and fill factor (FF), limiting their application in tandem solar cells. Here, we propose using the fullerene ICBA as the electron charge transporting layer (ETL), forming a better interfacial contact and enhancing the internal quasi-Fermi level splitting (QFLS). A further reduction of VOC losses of around 0.1 V was achieved by an ultrathin phenethylammonium chloride (PEACl) layer between the perovskite and the ETL. We precisely study the VOC improvement and find that passivation of surface recombination contributes only 20 mV, while more importantly, a major increase of 80 mV is achieved by dedoping the perovskite surface, which removes a non-negligible electron extraction barrier. Our results give helpful direction regarding how to further improve VOC in p-i-n perovskite cells.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00173

Chinese Library Classification Number:

Citation Information:

CsPbI2Br is an attractive photovoltaic material due to its promising optoelectronic properties. However, the corresponding perovskite solar cells (PSCs) with p-i-n configuration suffer from low open-circuit voltage (VOC) and fill factor (FF), limiting their application in tandem solar cells. Here, we propose using the fullerene ICBA as the electron charge transporting layer (ETL), forming a better interfacial contact and enhancing the internal quasi-Fermi level splitting (QFLS). A further reduction of VOC losses of around 0.1 V was achieved by an ultrathin phenethylammonium chloride (PEACl) layer between the perovskite and the ETL. We precisely study the VOC improvement and find that passivation of surface recombination contributes only 20 mV, while more importantly, a major increase of 80 mV is achieved by dedoping the perovskite surface, which removes a non-negligible electron extraction barrier. Our results give helpful direction regarding how to further improve VOC in p-i-n perovskite cells.

quote

GB/T 7714-2015 [1] Zijian Peng, Jingjing Tian, Kaicheng Zhang, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00173.
MLA [1] Zijian Peng, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00173.
APA [1] Zijian Peng, Jingjing Tian, Kaicheng Zhang, Albert These, Zhiqiang Xie, Yicheng Zhao, Andres Osvet, Fei Guo, Larry Lüer, Ning Li, & Christoph J. Brabec. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00173
IEEE [1] Zijian Peng, Jingjing Tian, Kaicheng Zhang, Albert These, Zhiqiang Xie, Yicheng Zhao, Andres Osvet, Fei Guo, Larry Lüer, Ning Li, and Christoph J. Brabec, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00173.