Flexible Bioinspired Ternary Nanocomposites Based on Carboxymethyl Cellulose/Nanoclay/Graphene Oxide AITranslate
Abstract AITranslate
Nacre is a prime example of a natural nanocomposite and an ideal motivation for nacre-mimetic materials. Natural nacre is a ternary nanocomposite made of aragonite platelets/chitin nanofibrils/protein and exhibits a combination of high tensile strength, stiffness, and toughness. Inspired by nacre, we developed ternary-bioinspired nanocomposites based on sodium carboxymethyl cellulose (CMC)/nanoclay platelets (SUM)/graphene oxide (GO) nanosheets via a water-borne evaporation-induced self-assembly technique. Structural characterizations of the layered nanocomposite films were done by FE-SEM, EDS, FTIR, RAMAN, XRD, and XPS. The mechanical properties of the nanocomposites were studied using a universal tensile tester, and the thermal behavior was analyzed using TGA. These ternary nacre-mimetics demonstrate high strength and flexibility via synergistic toughening from nanoclay platelets and graphene oxide as well as efficient interfacial stress transfer. The best synergistic improvement was obtained with CMC/SUM/GO-II ternary nanocomposite exhibiting a tensile strength, Young’s modulus, and toughness of 105 ± 12 MPa, 9.4 ± 0.3 GPa, and 6.2 ± 1.3 MJ/m3, respectively. These reported values are much superior to those of their corresponding binary (CMC/SUM and CMC/GO) nanocomposites as well as other previously reported un-cross-linked polymer/nanoclay or polymer/GO binary layered nanocomposites. Moreover, the tensile strength and toughness of CMC/SUM/GO-II nanocomposites are simultaneously 1.3 and 3.5 times higher as compared to natural nacre. In terms of functionality, these nanocomposites have shown shape-persistent, fire-blocking, and self-extinguishing properties. Hence, our study provides useful guidelines for designing and constructing future high-performance ternary-bioinspired materials, which can be applied as self-standing, ecofriendly, strong, and flexible materials for various applications like aerospace, flexible electronics, structural, and barrier materials.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.9b00245
Chinese Library Classification Number:
Citation Information:
Nacre is a prime example of a natural nanocomposite and an ideal motivation for nacre-mimetic materials. Natural nacre is a ternary nanocomposite made of aragonite platelets/chitin nanofibrils/protein and exhibits a combination of high tensile strength, stiffness, and toughness. Inspired by nacre, we developed ternary-bioinspired nanocomposites based on sodium carboxymethyl cellulose (CMC)/nanoclay platelets (SUM)/graphene oxide (GO) nanosheets via a water-borne evaporation-induced self-assembly technique. Structural characterizations of the layered nanocomposite films were done by FE-SEM, EDS, FTIR, RAMAN, XRD, and XPS. The mechanical properties of the nanocomposites were studied using a universal tensile tester, and the thermal behavior was analyzed using TGA. These ternary nacre-mimetics demonstrate high strength and flexibility via synergistic toughening from nanoclay platelets and graphene oxide as well as efficient interfacial stress transfer. The best synergistic improvement was obtained with CMC/SUM/GO-II ternary nanocomposite exhibiting a tensile strength, Young’s modulus, and toughness of 105 ± 12 MPa, 9.4 ± 0.3 GPa, and 6.2 ± 1.3 MJ/m3, respectively. These reported values are much superior to those of their corresponding binary (CMC/SUM and CMC/GO) nanocomposites as well as other previously reported un-cross-linked polymer/nanoclay or polymer/GO binary layered nanocomposites. Moreover, the tensile strength and toughness of CMC/SUM/GO-II nanocomposites are simultaneously 1.3 and 3.5 times higher as compared to natural nacre. In terms of functionality, these nanocomposites have shown shape-persistent, fire-blocking, and self-extinguishing properties. Hence, our study provides useful guidelines for designing and constructing future high-performance ternary-bioinspired materials, which can be applied as self-standing, ecofriendly, strong, and flexible materials for various applications like aerospace, flexible electronics, structural, and barrier materials.
quote
| GB/T 7714-2015 | [1] Paramita Das, Van Cuong Mai, Hongwei Duan. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00245. |
| MLA | [1] Paramita Das, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00245. |
| APA | [1] Paramita Das, Van Cuong Mai, & Hongwei Duan. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00245 |
| IEEE | [1] Paramita Das, Van Cuong Mai, and Hongwei Duan, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00245. keywords: {synergistic toughening;nacre;clay;graphene oxide;ternary nanocomposites;bioinspired materials} |