daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

An Effective and Reusable Hyperbranched Polymer Immobilized Rhodium Catalyst for the Hydroformylation of Olefins AITranslate

Department of Chemistry, KU Leuven; University of Siena;Laboratory of Green Synthetic Organic Chemistry; University of Siena;Department of Chemistry, KU Leuven;Laboratory of Green Synthetic Organic Chemistry;Department of Chemistry, KU Leuven
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Hydroformylation remains the most applied industrial process to produce aldehydes. Much research has been devoted to developing new catalyst systems since aldehydes are highly desired. Supported metal catalyst complexes have drawn renewed attention due to an increased interest in benign and environmental processes. In this paper, NiXantphos has been immobilized on hyperbranched poly(arylene oxindole) supports, different in linker, via a one-step postfunctionalization. Two heterogeneous hyperbranched poly(arylene oxindole) supported NiXantphos ligands were evaluated in the microwave-assisted rhodium-catalyzed hydroformylation of olefins. After selection of the best reaction conditions, a variety of functionalized olefins were successfully converted into the desired linear aldehydes working under milder conditions compared to known processes, in terms of syngas pressure (4.8 bar), temperature (75 °C), and reaction times (20 min). The increased activity might emanate from a positive dendritic effect unique to the dendritic nature of the support. Furthermore, the catalyst system was successfully recovered and reused without a decrease in activity or regioselectivity, thus demonstrating to be a valid alternative to classical homogeneous procedures.

KeyWords AITranslate

heterogeneous hydroformylation microwave hyperbranched polymers rhodium Xantphos hyperbranched poly(arylene oxindole) Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00240

Chinese Library Classification Number:

Citation Information:

Hydroformylation remains the most applied industrial process to produce aldehydes. Much research has been devoted to developing new catalyst systems since aldehydes are highly desired. Supported metal catalyst complexes have drawn renewed attention due to an increased interest in benign and environmental processes. In this paper, NiXantphos has been immobilized on hyperbranched poly(arylene oxindole) supports, different in linker, via a one-step postfunctionalization. Two heterogeneous hyperbranched poly(arylene oxindole) supported NiXantphos ligands were evaluated in the microwave-assisted rhodium-catalyzed hydroformylation of olefins. After selection of the best reaction conditions, a variety of functionalized olefins were successfully converted into the desired linear aldehydes working under milder conditions compared to known processes, in terms of syngas pressure (4.8 bar), temperature (75 °C), and reaction times (20 min). The increased activity might emanate from a positive dendritic effect unique to the dendritic nature of the support. Furthermore, the catalyst system was successfully recovered and reused without a decrease in activity or regioselectivity, thus demonstrating to be a valid alternative to classical homogeneous procedures.

quote

GB/T 7714-2015 [1] Thomas Verheyen, Niccolò Santillo, Davide Marinelli, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00240.
MLA [1] Thomas Verheyen, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00240.
APA [1] Thomas Verheyen, Niccolò Santillo, Davide Marinelli, Elena Petricci, Wim M. De Borggraeve, Luigi Vaccaro, & Mario Smet. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00240
IEEE [1] Thomas Verheyen, Niccolò Santillo, Davide Marinelli, Elena Petricci, Wim M. De Borggraeve, Luigi Vaccaro, and Mario Smet, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00240. keywords: {heterogeneous hydroformylation;microwave;hyperbranched polymers;rhodium;Xantphos;hyperbranched poly(arylene oxindole);Show More}