Cellulose/Poly(meta-phenylene isophthalamide) Light-Management Films with High Antiultraviolet and Tunable Haze Performances AITranslate

Qilu University of Technology (Shandong Academy of Sciences); Qilu University of Technology (Shandong Academy of Sciences); Qilu University of Technology (Shandong Academy of Sciences); Qilu University of Technology (Shandong Academy of Sciences)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Light-management films are usually fabricated from the petrochemical-based polymers, and developing renewable and biodegradable cellulose-based light-management films with high transparence, tunable haze, and UV-blocking capacity by a facile and large-scale production method is still challenging. Herein, cellulose/poly(meta-phenylene isophthalamide) (PMIA) light-management films were manufactured by simple blending, which was fit for the large-scale production of cellulose/PMIA films. It was found that the cellulose/PMIA composite films showed tunable haze (14–55%), high transparence (>78%), UV-blocking capacity, and irradiation stability. In addition, the elongation at break and tensile strength of the composite film can be improved to 23.78% and 55.90 MPa compared to those of the native cellulose film (21.94% and 45.83 MPa), ascribed to copious hydrogen bonds between PMIA and cellulose molecules. Hence, the cellulose/PMIA light-management films with enhanced optical and mechanical properties were fabricated successfully, and they showed great potential in flexible displays and energy-efficient buildings.

KeyWords AITranslate

cellulose composite film light management haze UV shielding ionic liquid
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01325

Chinese Library Classification Number:

Citation Information:

Light-management films are usually fabricated from the petrochemical-based polymers, and developing renewable and biodegradable cellulose-based light-management films with high transparence, tunable haze, and UV-blocking capacity by a facile and large-scale production method is still challenging. Herein, cellulose/poly(meta-phenylene isophthalamide) (PMIA) light-management films were manufactured by simple blending, which was fit for the large-scale production of cellulose/PMIA films. It was found that the cellulose/PMIA composite films showed tunable haze (14–55%), high transparence (>78%), UV-blocking capacity, and irradiation stability. In addition, the elongation at break and tensile strength of the composite film can be improved to 23.78% and 55.90 MPa compared to those of the native cellulose film (21.94% and 45.83 MPa), ascribed to copious hydrogen bonds between PMIA and cellulose molecules. Hence, the cellulose/PMIA light-management films with enhanced optical and mechanical properties were fabricated successfully, and they showed great potential in flexible displays and energy-efficient buildings.

quote

GB/T 7714-2015 [1] Guangmei Xia, Xiaoqian Ji, Jianfeng Peng, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01325.
MLA [1] Guangmei Xia, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01325.
APA [1] Guangmei Xia, Xiaoqian Ji, Jianfeng Peng, & Xingxiang Ji. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01325
IEEE [1] Guangmei Xia, Xiaoqian Ji, Jianfeng Peng, and Xingxiang Ji, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01325. keywords: {cellulose composite film;light management;haze;UV shielding;ionic liquid}