Poly(2-methacryloyloxyethyl phosphorylcholine) Grafted Bioprosthetic Heart Valve Exhibited Improved Antithrombogenicity and Anticalcification Properties AITranslate

Sichuan University; Sichuan University; Sichuan University; Sichuan University; Sichuan University; Sichuan University; Sichuan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Replacing diseased valves with bioprosthetic heart valves (BHVs) is an increasingly recognized treatment for valvular heart disease (VHD) due to the increasing application of transcatheter aortic valve replacement (TAVR) techniques. However, the dysfunction and structural valvular degeneration (SVD) of BHVs caused by the drawbacks of the traditional glutaraldehyde cross-linking strategy including thrombosis, cytotoxicity, and calcification could shorten the lifespan of BHVs. In this study, a modification strategy for BHVs based on cocrosslinking and copolymerization was developed. Decellularized porcine pericardium and partially methacrylated poly-ε-lysine were first cocrosslinked by glutaraldehyde to achieve the cross-linking and methacrylation of porcine pericardium simultaneously, and then methacrylated modified pericardium was copolymerized with zwitterionic monomer 2-methacryloyloxyethyl phosphorylcholine (MPC) to prepare poly-MPC grafted porcine pericardium (GM). GM exhibited improved endothelialial cells’ proliferation compared with traditional glutaraldehyde cross-linked pericardium (GA) (3.67-fold higher than GA after a 3-day incubation). The platelets’ adhesion test demonstrated the superiority of GM in resistance of platelet adhesion, where the platelet adhered on the surface of GM decreased by levels of approximately 75% compared with GA. Meanwhile, the results of 60-day and 150-day rat subcutaneous implantation demonstrated that GM exhibited improved anticalcification property than GA (1.6 ± 0.4 μg/mg versus 224 ± 15 μg/mg and 3.1 ± 0.5 μg/mg versus 252 ± 15 μg/mg respectively). All the results show that our modification strategy may have the potential for clinical application.

KeyWords AITranslate

bioprosthetic heart valves 2methacryloyloxyethyl phosphorylcholine copolymerization anticalcification antithrombogenicity
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01334

Chinese Library Classification Number:

Citation Information:

Replacing diseased valves with bioprosthetic heart valves (BHVs) is an increasingly recognized treatment for valvular heart disease (VHD) due to the increasing application of transcatheter aortic valve replacement (TAVR) techniques. However, the dysfunction and structural valvular degeneration (SVD) of BHVs caused by the drawbacks of the traditional glutaraldehyde cross-linking strategy including thrombosis, cytotoxicity, and calcification could shorten the lifespan of BHVs. In this study, a modification strategy for BHVs based on cocrosslinking and copolymerization was developed. Decellularized porcine pericardium and partially methacrylated poly-ε-lysine were first cocrosslinked by glutaraldehyde to achieve the cross-linking and methacrylation of porcine pericardium simultaneously, and then methacrylated modified pericardium was copolymerized with zwitterionic monomer 2-methacryloyloxyethyl phosphorylcholine (MPC) to prepare poly-MPC grafted porcine pericardium (GM). GM exhibited improved endothelialial cells’ proliferation compared with traditional glutaraldehyde cross-linked pericardium (GA) (3.67-fold higher than GA after a 3-day incubation). The platelets’ adhesion test demonstrated the superiority of GM in resistance of platelet adhesion, where the platelet adhered on the surface of GM decreased by levels of approximately 75% compared with GA. Meanwhile, the results of 60-day and 150-day rat subcutaneous implantation demonstrated that GM exhibited improved anticalcification property than GA (1.6 ± 0.4 μg/mg versus 224 ± 15 μg/mg and 3.1 ± 0.5 μg/mg versus 252 ± 15 μg/mg respectively). All the results show that our modification strategy may have the potential for clinical application.

quote

GB/T 7714-2015 [1] Xueyu Huang, Cheng Zheng, Kailei Ding, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01334.
MLA [1] Xueyu Huang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01334.
APA [1] Xueyu Huang, Cheng Zheng, Kailei Ding, Shumang Zhang, Qingrong Wei, Li Yang, & Yunbing Wang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01334
IEEE [1] Xueyu Huang, Cheng Zheng, Kailei Ding, Shumang Zhang, Qingrong Wei, Li Yang, and Yunbing Wang, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01334. keywords: {bioprosthetic heart valves;2methacryloyloxyethyl phosphorylcholine;copolymerization;anticalcification;antithrombogenicity}