Revealing Compositional Evolution of PdAu Electrocatalyst by Atom Probe Tomography AITranslate
Abstract AITranslate
Pd-based electro-catalysts are a key component to improve the methanol oxidation reaction (MOR) kinetics from alcohol fuel cells. However, the performance of such catalysts is degraded over time. To understand the microstructural/atomic scale chemical changes responsible for such an effect, scanning (transmission) electron microscopy measurements and atom probe tomography were performed after accelerated degradation tests. No morphological changes are observed after 1000 MOR cycles. In contrast, (1) Pd and B are leached from PdAu nanoparticles and (2) Au-rich regions are formed at the surface of the catalyst. These insights highlight the importance of understanding the chemical modification occurring upon MOR to design new catalysts.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.3c00911
Chinese Library Classification Number:
Citation Information:
Pd-based electro-catalysts are a key component to improve the methanol oxidation reaction (MOR) kinetics from alcohol fuel cells. However, the performance of such catalysts is degraded over time. To understand the microstructural/atomic scale chemical changes responsible for such an effect, scanning (transmission) electron microscopy measurements and atom probe tomography were performed after accelerated degradation tests. No morphological changes are observed after 1000 MOR cycles. In contrast, (1) Pd and B are leached from PdAu nanoparticles and (2) Au-rich regions are formed at the surface of the catalyst. These insights highlight the importance of understanding the chemical modification occurring upon MOR to design new catalysts.
quote
| GB/T 7714-2015 | [1] Leonardo Shoji Aota, Chanwon Jung, Siyuan Zhang, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00911. |
| MLA | [1] Leonardo Shoji Aota, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00911. |
| APA | [1] Leonardo Shoji Aota, Chanwon Jung, Siyuan Zhang, SeHo Kim, & Baptiste Gault. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00911 |
| IEEE | [1] Leonardo Shoji Aota, Chanwon Jung, Siyuan Zhang, SeHo Kim, and Baptiste Gault, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00911. |