Reversible White-Light-Driven Photochromic Polymer Hydrogels with High Stretchability and Adhesiveness AITranslate
Abstract AITranslate
Photochromic materials that reversibly change color by light stimulus are of interest for developing sensors and optoelectronics. A design of Ag+-containing photochromic polymer hydrogel showing reversible photochromism, high stretchability, and high adhesiveness is reported. The polymer hydrogel is fabricated using the Ag+/ammonium persulfate (APS) fast gelation system, which initiates the fast gelation of the acrylic acid (AA) and 3-iminodiacetate-2-hydroxypropyl methacrylate (IDHPMA) aqueous solution. The iminodiacetate (IDA) ligands from the copolymer bind with Ag+ ions to form Ag+–IDA coordination cross-links, contributing to the high stretchability of the hydrogel. The Ag+–IDA complexes also impart a high adhesion performance to the hydrogel through the formation of Mn+–IDA complexes on various metal surfaces. The Ag+ ions in the hydrogel undergo a reversible transition between the ionic and Ag nanoparticle states when subjected to switchable white-light irradiation and incubation in the dark. It is demonstrated that this photochromic hydrogel was suitable for photopatterning with a controllable storage time. This photochromic hydrogel illustrates a pathway to make soft wearable devices for controllable information storage and anticounterfeiting, where high stretchability and adhesiveness are required.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01383
Chinese Library Classification Number:
Citation Information:
Photochromic materials that reversibly change color by light stimulus are of interest for developing sensors and optoelectronics. A design of Ag+-containing photochromic polymer hydrogel showing reversible photochromism, high stretchability, and high adhesiveness is reported. The polymer hydrogel is fabricated using the Ag+/ammonium persulfate (APS) fast gelation system, which initiates the fast gelation of the acrylic acid (AA) and 3-iminodiacetate-2-hydroxypropyl methacrylate (IDHPMA) aqueous solution. The iminodiacetate (IDA) ligands from the copolymer bind with Ag+ ions to form Ag+–IDA coordination cross-links, contributing to the high stretchability of the hydrogel. The Ag+–IDA complexes also impart a high adhesion performance to the hydrogel through the formation of Mn+–IDA complexes on various metal surfaces. The Ag+ ions in the hydrogel undergo a reversible transition between the ionic and Ag nanoparticle states when subjected to switchable white-light irradiation and incubation in the dark. It is demonstrated that this photochromic hydrogel was suitable for photopatterning with a controllable storage time. This photochromic hydrogel illustrates a pathway to make soft wearable devices for controllable information storage and anticounterfeiting, where high stretchability and adhesiveness are required.
quote
| GB/T 7714-2015 | [1] Yongqi Liu, Jingtao Jiang, Xiuyu Huang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01383. |
| MLA | [1] Yongqi Liu, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01383. |
| APA | [1] Yongqi Liu, Jingtao Jiang, Xiuyu Huang, Jingzhi Tang, Qiuli Tan, Yang Chen, Youwei Xiao, Xiaoli Wu, & Gengsheng Weng. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01383 |
| IEEE | [1] Yongqi Liu, Jingtao Jiang, Xiuyu Huang, Jingzhi Tang, Qiuli Tan, Yang Chen, Youwei Xiao, Xiaoli Wu, and Gengsheng Weng, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01383. keywords: {photochromic hydrogel;dynamic coordination;highly stretchable;adhesion;silver ion} |