daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Removal of phenazopyridine as a pharmacological contaminant using nanoporous metal/covalent-organic frameworks (MOF/COF) adsorbent AITranslate

Amirkabir University of Technology (Tehran Polytechnic); Shiraz University; Iran University of Science and Technology; Amirkabir University of Technology (Tehran Polytechnic);Institut national de la recherché (INRS), Centre Énergie Matériaux Télécommunications (EMT); Amirkabir University of Technology (Tehran Polytechnic); University of Technology Sydney
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This study is aimed at employing the Molecular Dynamics simulations to assess the phenazopyridine (PHP) adsorption, an analgesic drug, on three new metal-organic frameworks (MOFs); IRMOF-16, HKUST-1, and ZIF-8, with excellent behavior in π−π stacking, H-bonding, and electrostatic interactions. To further decipher the adsorption mechanism of PHP on MOFs, coarse-grained (CG) simulations and density functional theory (DFT) calculations were also exploited. Simulations revealed the PHP adsorption intensity of around 100%, 60%, and 40% by IRMOF-16, HKUST-1, and ZIF-8, respectively. Moreover, CG simulations and DFT calculation validated the superior PHP adsorption capacity of IRMOF-16 with the energy value of -343.4 kJ/mol and -1.53 eV, respectively. Furthermore, the PHP adsorption capability of IRMOF-16 was scrutinized under three distinct modifications: functionalization with hydroxyl functional group, tuning porosity size, and hybrid framework formation with DAAQ-TFP Covalent Organic Frame (COF). Interestingly, the modification of IRMOF-16 with hydroxyl groups and grafting with the COF led to considerably better performance in removing PHP, since their modifications increased the negative net charge of the surface, resulting in greater interactions with the positively charged PHP molecules. Furthermore, enlarging the IRMOF-16 pore size relatively reduced the adsorption functionality, due to the limited interactions of PHPs with available active sites. Graphical abstract Download : Download high-res image (212KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2021.101196

Chinese Library Classification Number:

Citation Information:

This study is aimed at employing the Molecular Dynamics simulations to assess the phenazopyridine (PHP) adsorption, an analgesic drug, on three new metal-organic frameworks (MOFs); IRMOF-16, HKUST-1, and ZIF-8, with excellent behavior in π−π stacking, H-bonding, and electrostatic interactions. To further decipher the adsorption mechanism of PHP on MOFs, coarse-grained (CG) simulations and density functional theory (DFT) calculations were also exploited. Simulations revealed the PHP adsorption intensity of around 100%, 60%, and 40% by IRMOF-16, HKUST-1, and ZIF-8, respectively. Moreover, CG simulations and DFT calculation validated the superior PHP adsorption capacity of IRMOF-16 with the energy value of -343.4 kJ/mol and -1.53 eV, respectively. Furthermore, the PHP adsorption capability of IRMOF-16 was scrutinized under three distinct modifications: functionalization with hydroxyl functional group, tuning porosity size, and hybrid framework formation with DAAQ-TFP Covalent Organic Frame (COF). Interestingly, the modification of IRMOF-16 with hydroxyl groups and grafting with the COF led to considerably better performance in removing PHP, since their modifications increased the negative net charge of the surface, resulting in greater interactions with the positively charged PHP molecules. Furthermore, enlarging the IRMOF-16 pore size relatively reduced the adsorption functionality, due to the limited interactions of PHPs with available active sites. Graphical abstract Download : Download high-res image (212KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Mohammad Khedri, Reza Maleki, Sina Ghaemi Khiavi, et al. Applied Materials Today, 2021(25). DOI:10.1016/j.apmt.2021.101196.
MLA [1] Mohammad Khedri, et al., Applied Materials Today, no. 25, 2021, https://doi.org/10.1016/j.apmt.2021.101196.
APA [1] Mohammad Khedri, Reza Maleki, Sina Ghaemi Khiavi, Mehdi Ghasemi, Ebrahim Ghasemy, Ahmad Miri Jahromi, & Amir Razmjou. (2021). Applied Materials Today(25). https://doi.org/10.1016/j.apmt.2021.101196
IEEE [1] Mohammad Khedri, Reza Maleki, Sina Ghaemi Khiavi, Mehdi Ghasemi, Ebrahim Ghasemy, Ahmad Miri Jahromi, and Amir Razmjou, Applied Materials Today, no. 25, 2021, doi: 10.1016/j.apmt.2021.101196.