Antibacterial Cellulose Fibers Spun from Ionic Liquid and Enriched with Plant Essential Oils AITranslate
Abstract AITranslate
The COVID-19 outbreak has seen the widespread use of personal protective equipment, especially antibacterial fibers. In this work, ionic liquid (IL) is used as a solvent to fabricate antibacterial fibers combining plant essential oils (PEOs) with cellulose. PEOs are buried in microcapsules first or mixed directly with IL-cellulose spinning dopes to prepare a series of composite fibers. The internal structures, surface and cross morphologies, thermal stability, mechanical properties, antibacterial activity, washing stability, and biocompatibility of these fibers are investigated and analyzed in-depth further. Artemisia microcapsule fiber (AMC-RCF) with a break strength of 30.07 MPa is obtained. Besides, the antibacterial activity rates of AMC-RCF against Escherichia coli and Staphylococcus aureus are 89.8 and 97.8%, and the fibers still have a long-lasting antibacterial effect after 30 standard washes. Furthermore, the antibacterial fibers exhibit excellent biocompatibility. This research provides a green approach for the fabrication of the antibacterial fibers with long-lasting antibacterial activity and good biocompatibility.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c01018
Chinese Library Classification Number:
Citation Information:
The COVID-19 outbreak has seen the widespread use of personal protective equipment, especially antibacterial fibers. In this work, ionic liquid (IL) is used as a solvent to fabricate antibacterial fibers combining plant essential oils (PEOs) with cellulose. PEOs are buried in microcapsules first or mixed directly with IL-cellulose spinning dopes to prepare a series of composite fibers. The internal structures, surface and cross morphologies, thermal stability, mechanical properties, antibacterial activity, washing stability, and biocompatibility of these fibers are investigated and analyzed in-depth further. Artemisia microcapsule fiber (AMC-RCF) with a break strength of 30.07 MPa is obtained. Besides, the antibacterial activity rates of AMC-RCF against Escherichia coli and Staphylococcus aureus are 89.8 and 97.8%, and the fibers still have a long-lasting antibacterial effect after 30 standard washes. Furthermore, the antibacterial fibers exhibit excellent biocompatibility. This research provides a green approach for the fabrication of the antibacterial fibers with long-lasting antibacterial activity and good biocompatibility.
quote
| GB/T 7714-2015 | [1] Le Zhou, Xinxin Li, Zhaoqing Kang, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01018. |
| MLA | [1] Le Zhou, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01018. |
| APA | [1] Le Zhou, Xinxin Li, Zhaoqing Kang, Xue Liu, Qiongguang Li, Liangyu Ma, Hongshuai Gao, & Yi Nie. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01018 |
| IEEE | [1] Le Zhou, Xinxin Li, Zhaoqing Kang, Xue Liu, Qiongguang Li, Liangyu Ma, Hongshuai Gao, and Yi Nie, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01018. keywords: {antibacterial fibers;plant essential oils;microcapsules;ionic liquids;regenerated cellulose fibers} |