daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Light Makes Right: Laser Polishing for Surface Modification of Perovskite Solar Cells AITranslate

University of Stuttgart; University of Stuttgart; University of Luxembourg; Universidad de Valencia; University of Stuttgart; Universidad de Valencia; University of Stuttgart; Brandenburg University of Technology Cottbus-Senftenberg; University of Stuttgart; Brandenburg University of Technology Cottbus-Senftenberg; University of Luxembourg; University of Stuttgart
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Interface engineering is a common strategy for passivating surface defects to attain open circuit voltages (Voc) in perovskite solar cells (PSCs). In this work, we introduce the concept of polishing a perovskite thin-film surface using a nanosecond (ns) pulsed ultraviolet laser to reduce surface defects, such as dangling bonds, undesirable phases, and suboptimal stoichiometry. A careful control of laser energy and scanning speed improves the photophysical properties of the surface without compromising the thickness. Using laser polishing, a Voc of 1.21 V is achieved for planar PSCs with a triple cation composition, showing an improved perovskite/hole transport interface by mitigating surface recombination losses. We measure an efficiency boost from 18.0% to 19.3% with improved stability of up to 1000 h. The results open the door to a new class of surface modification using lasers for interface passivation in well-controllable, automated, scalable, and solvent-free surface treatments.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.3c00469

Chinese Library Classification Number:

Citation Information:

Interface engineering is a common strategy for passivating surface defects to attain open circuit voltages (Voc) in perovskite solar cells (PSCs). In this work, we introduce the concept of polishing a perovskite thin-film surface using a nanosecond (ns) pulsed ultraviolet laser to reduce surface defects, such as dangling bonds, undesirable phases, and suboptimal stoichiometry. A careful control of laser energy and scanning speed improves the photophysical properties of the surface without compromising the thickness. Using laser polishing, a Voc of 1.21 V is achieved for planar PSCs with a triple cation composition, showing an improved perovskite/hole transport interface by mitigating surface recombination losses. We measure an efficiency boost from 18.0% to 19.3% with improved stability of up to 1000 h. The results open the door to a new class of surface modification using lasers for interface passivation in well-controllable, automated, scalable, and solvent-free surface treatments.

quote

GB/T 7714-2015 [1] Mayank Kedia, Monika Rai, Himanshu Phirke, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.3c00469.
MLA [1] Mayank Kedia, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.3c00469.
APA [1] Mayank Kedia, Monika Rai, Himanshu Phirke, Clara A Aranda, Chittaranjan Das, Vladimir Chirvony, Stephan Boehringer, Małgorzata Kot, Mahdi Malekshahi Byranvand, Jan Ingo Flege, Alex Redinger, & Michael Saliba. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.3c00469
IEEE [1] Mayank Kedia, Monika Rai, Himanshu Phirke, Clara A Aranda, Chittaranjan Das, Vladimir Chirvony, Stephan Boehringer, Małgorzata Kot, Mahdi Malekshahi Byranvand, Jan Ingo Flege, Alex Redinger, and Michael Saliba, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.3c00469.