Lightweight Antistatic Thermoplastic Elastomer Blend Foam: The Foaming Behavior and Mechanical Properties AITranslate

Qingdao University of Science and Technology; Qingdao University of Science and Technology; Qingdao University of Science and Technology; Qingdao University of Science and Technology; Qingdao University of Science and Technology; Qingdao University of Science and Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A thermoplastic polyester elastomer (TPEE) has been widely used because of its excellent impact resistance and resilience, but its melt viscosity is too low to be used in the supercritical foaming. In addition, TPEE easily generates static electricity accumulation during processing, which has a risk of fire. Herein, a thermoplastic polyamide elastomer (PEBAX) with permanent antistatic properties was blended with TPEE, and triglycidyl isocyanurate (TGIC) was used as a chain extender to improve the compatibility and melt strength of the blends. Then, the TPEE/PEBAX blends were foamed by supercritical N2, and the cell structure and mechanical and antistatic properties of the blend foam were analyzed at a density of 0.1 ± 0.001 g/cm3. The results showed that when the blending ratio of TPEE/PEBAX was 70/30, the blend foam with a uniform cell structure had the most excellent mechanical properties. The resilience and elongation at break reached 83 and 850.3%, respectively. In addition, the surface resistivity and volume resistivity were 3.21 × 109 Ω and 7.35 × 109 Ω·cm, respectively, which were significantly lower than those of the IEC 61340 standard.

KeyWords AITranslate

antistatic TPEE PEBAX chain extension supercritical foaming
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00443

Chinese Library Classification Number:

Citation Information:

A thermoplastic polyester elastomer (TPEE) has been widely used because of its excellent impact resistance and resilience, but its melt viscosity is too low to be used in the supercritical foaming. In addition, TPEE easily generates static electricity accumulation during processing, which has a risk of fire. Herein, a thermoplastic polyamide elastomer (PEBAX) with permanent antistatic properties was blended with TPEE, and triglycidyl isocyanurate (TGIC) was used as a chain extender to improve the compatibility and melt strength of the blends. Then, the TPEE/PEBAX blends were foamed by supercritical N2, and the cell structure and mechanical and antistatic properties of the blend foam were analyzed at a density of 0.1 ± 0.001 g/cm3. The results showed that when the blending ratio of TPEE/PEBAX was 70/30, the blend foam with a uniform cell structure had the most excellent mechanical properties. The resilience and elongation at break reached 83 and 850.3%, respectively. In addition, the surface resistivity and volume resistivity were 3.21 × 109 Ω and 7.35 × 109 Ω·cm, respectively, which were significantly lower than those of the IEC 61340 standard.

quote

GB/T 7714-2015 [1] Wenzhang Huang, Leilei Yu, Zhen Yu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00443.
MLA [1] Wenzhang Huang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00443.
APA [1] Wenzhang Huang, Leilei Yu, Zhen Yu, Lijuan Yang, Shibao Wen, & Zhen Xiu Zhang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00443
IEEE [1] Wenzhang Huang, Leilei Yu, Zhen Yu, Lijuan Yang, Shibao Wen, and Zhen Xiu Zhang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00443. keywords: {antistatic;TPEE;PEBAX;chain extension;supercritical foaming}