Organic–Inorganic Polyimides with POSS Cages in the Main Chains: An Impact of POSS R Groups on Morphologies and Properties AITranslate

Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Two well-defined POSS diamines were synthesized with phenyl (Ph) and iso-butyl (i-Bu) POSS trisilanols as the starting compounds. This approach involves the protection and deprotection of silanol hydroxyl groups with phenylboronic acid and pinacol, followed by the silylation of silanol hydroxyl groups with mono- and dichlorosilanes. With this route of synthesis, two well-defined divinyl POSS macromers were obtained, as evidenced by 1H, 29Si NMR, and mass spectroscopy. These two divinyl POSS macromers were further functionalized into well-defined POSS diamines via the Heck reaction with p-bromoaniline. The successful synthesis of POSS diamines enabled the synthesis of organic–inorganic polyimides with the POSS cages in the main chains. More importantly, the syntheses of these two POSS diamines allowed the examination of the effect of POSS R groups (i.e., Ph and i-Bu) on the morphologies and thermomechanical and dielectric properties of organic–inorganic polyimides. Notably, the types of POSS R groups exerted a profound impact on the morphologies and properties of the organic–inorganic polyimides.

KeyWords AITranslate

polyimide POSS microphaseseparation thermomechanical properties dielectric properties
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00456

Chinese Library Classification Number:

Citation Information:

Two well-defined POSS diamines were synthesized with phenyl (Ph) and iso-butyl (i-Bu) POSS trisilanols as the starting compounds. This approach involves the protection and deprotection of silanol hydroxyl groups with phenylboronic acid and pinacol, followed by the silylation of silanol hydroxyl groups with mono- and dichlorosilanes. With this route of synthesis, two well-defined divinyl POSS macromers were obtained, as evidenced by 1H, 29Si NMR, and mass spectroscopy. These two divinyl POSS macromers were further functionalized into well-defined POSS diamines via the Heck reaction with p-bromoaniline. The successful synthesis of POSS diamines enabled the synthesis of organic–inorganic polyimides with the POSS cages in the main chains. More importantly, the syntheses of these two POSS diamines allowed the examination of the effect of POSS R groups (i.e., Ph and i-Bu) on the morphologies and thermomechanical and dielectric properties of organic–inorganic polyimides. Notably, the types of POSS R groups exerted a profound impact on the morphologies and properties of the organic–inorganic polyimides.

quote

GB/T 7714-2015 [1] Huaming Wang, Guohua Hang, Jiawei Hu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00456.
MLA [1] Huaming Wang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00456.
APA [1] Huaming Wang, Guohua Hang, Jiawei Hu, Yuan Gao, Lei Li, & Sixun Zheng. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00456
IEEE [1] Huaming Wang, Guohua Hang, Jiawei Hu, Yuan Gao, Lei Li, and Sixun Zheng, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00456. keywords: {polyimide;POSS;microphaseseparation;thermomechanical properties;dielectric properties}